H59 Brass Round Bar: Composition, Machining and Buying Guide

H59 brass round bar is a hot-extruded or cold-drawn copper-zinc bar with a nominal copper content of 57–60%. It sits between the cheaper, harder brasses and the more ductile 63/37 grades, which makes it a practical choice for machined fittings, threaded parts, bushes and decorative hardware where strength and cost matter more than maximum conductivity.

What H59 Brass Round Bar Is and Where It Is Used

H59 is a binary copper-zinc alloy. The “59” refers to the copper level, not to a hardness or a tensile grade. At roughly 59% copper the microstructure contains both alpha and beta phase, so the bar is stronger than single-phase 65/35 brass and responds well to hot working, while still being machinable at moderate speeds. It is not a free-cutting grade in the strict sense, because its lead level is capped as an impurity rather than added deliberately.

Typical uses fall into four groups. The first is plumbing and sanitary hardware: valve bodies, adapters, shower fittings, tap escutcheons and compression nuts. The second is general engineering: bushes, bearing sleeves, worm gears, brackets, spacer bars and small shafts. The third is electrical and thermal hardware where moderate conductivity is acceptable: terminal blocks, heat-sink studs, connector pins and switch parts. The fourth is decorative and architectural: baluster spindles, handrail inserts, furniture trim and signage frames that will be polished, lacquered or plated.

Buyers often confuse H59 bar with H59-1 bar. H59-1 is the leaded, free-cutting variant with deliberately added lead, usually 0.8–1.9%. It machines faster and produces shorter chips, but it is restricted in potable-water and food-contact applications and is harder to weld. H59, with lead treated only as a residual impurity, is the better choice when the part will be brazed, polished, plated or used near drinking water.

H59 brass round bar bundle in mill storage
H59 brass round bars stacked by diameter, with grade and size marked on the ends in marker pen.

Grade Designation and Chemical Composition

H59 is specified in China by GB/T 5231 (wrought copper and copper alloy grades) and corresponds broadly to the ISO CuZn40 family, although exact limits differ between standards. The table below shows the typical GB/T 5231 window for H59. Values are percentage by mass, with copper as the balance-determining element and zinc making up almost all of the remainder.

Element H59 range (%) Typical value (%) Effect on the bar
Cu 57.0–60.0 58.5 Sets conductivity, colour and corrosion behaviour
Zn Balance Remainder Raises strength; lowers melting point
Pb ≤ 0.50 0.05–0.30 Residual only; improves chip break at higher levels
Fe ≤ 0.30 0.10 Refines grain; excess forms hard inclusions
Sn ≤ 0.20 0.05 Residual; can raise strength slightly
Al ≤ 0.10 0.02 Deoxidiser; excess hurts hot ductility
Sb ≤ 0.01 trace Brittle intermetallic if uncontrolled
Bi ≤ 0.002 trace Hot-short cracking above limit
P ≤ 0.01 trace Residual; embrittles at higher levels
Total impurities ≤ 1.0 — Purchasing check point

Typical GB/T 5231 window for H59. Confirm the exact standard and limits on the mill certificate before releasing a pressure or potable-water part.

Mechanical Properties

H59 bar is normally supplied in the extruded (hot-worked) condition, sometimes designated M or R. Cold drawing to a smaller diameter raises strength and lowers elongation, and a light stress-relief anneal restores some ductility. The table gives typical ranges measured on 10–40 mm round bar at room temperature; they are design guidance, not a substitute for the mill’s own test report.

Property Extruded (M) Cold drawn + annealed Cold drawn hard
0.2% proof stress, Rp0.2 (MPa) 180–240 220–300 320–420
Tensile strength, Rm (MPa) 400–500 450–560 560–700
Elongation, A (%) 20–30 15–25 5–12
Hardness, HB 90–115 105–130 130–170
Electrical conductivity (% IACS) 25–29 25–29 24–28
Thermal conductivity (W/m·K) 90–110 90–110 85–105

Typical room-temperature values for H59 round bar. Hardness and strength rise with drawing reduction; confirm temper and test direction for critical parts.

Two practical consequences follow. First, if the drawing calls for a specific proof stress, state the temper and the test direction, because a cold-drawn 12 mm bar can be 40% stronger than the same alloy in the extruded condition. Second, H59 is not a high-temperature alloy: above about 200 °C the proof stress falls quickly, and prolonged service above 250 °C promotes grain growth and loss of ductility.

Dimensions, Tolerances and Supply Forms

H59 round bar is commonly produced from 3 mm to 100 mm diameter, with 6–60 mm being the stock range most mills hold. Larger sections are usually extruded and may be supplied in random length; smaller diameters are drawn in coils or straight lengths. The tolerance band depends on the standard and the drawing reduction, so a buyer should specify diameter, tolerance class, straightness and length rather than only the nominal size.

Feature Common range Typical tolerance Notes
Diameter 3–100 mm h9, h11 or ±0.05 mm Tight classes cost more; state if screw threads follow
Length 1–6 m +5 / 0 mm Random mill lengths are cheaper
Straightness — 0.5–2 mm per metre Needed for automatic lathes
Roundness — ≤ 50% of diameter tolerance Check on turned stock
Surface — Bright, pickled or peeled Peeling removes extrusion skin and defects
Ends — Saw cut, chamfered on request Chamfer reduces handling damage
Coil weight — 50–300 kg For diameters below 12 mm

Typical commercial windows. For threaded bar, specify the thread standard and allow the bar diameter to suit the thread root rather than the nominal thread size.

Surface condition deserves its own line on the purchase order. Extruded bar carries a thin oxide skin and may show die lines; peeled bar removes that skin and exposes sound metal, which is preferred for plating and for parts that will be polished. Pickled bar is cleaned chemically and is suitable for general machining, but it can hide shallow seams if the pickling is overdone. Never accept “bright” as a finish description without stating whether it is peeled, turned or chemically brightened.

H59 brass bar ends showing grade marking
Close view of H59 bar ends with handwritten grade marks; the bar surfaces are bright and free of visible seams.

How H59 Round Bar Is Made

The route starts with cathode copper and zinc ingot, melted in an induction furnace under a charcoal or borax cover to limit zinc loss. Phosphorus is used cautiously as a deoxidiser; residual phosphorus above about 0.01% is harmful, so the melt is usually killed with a small addition and then checked by spectrography before casting. The cast billet is homogenised, then extruded through a die at 700–800 °C into bar. Extrusion gives a sound, fine-grained core and is the cheapest way to make long lengths.

Smaller diameters are cold drawn from extruded rod through carbide dies, with interpass annealing to restore ductility. Drawing reduces diameter, improves roundness and raises strength. After the final pass the bar is straightened on a two-roll or rotary straightener, cut to length, and either left bright, peeled or pickled. Stress-relief annealing at 250–350 °C is used when the part must hold tolerance during machining, because cold drawing leaves a residual stress pattern that can bow a long bar after one side is milled.

The manufacturing details that most often cause complaints are straightness after cutting, residual stress and surface seams. A bar that is straight in the bundle can bow after sawing because the cut releases stress. A bar that looks clean can reveal a longitudinal seam after turning, especially if the extrusion billet had a shrinkage cavity. Both are controlled by billet quality, extrusion temperature and a peel pass, not by inspection alone.

Machining H59 Brass

H59 machines like a medium-strength brass. It is softer and more ductile than H59-1, so chips tend to be long and stringy. Use sharp, positive-rake carbide tooling with a polished rake face, high speed and moderate feed: for turning, 250–450 m/min surface speed and 0.08–0.20 mm/rev feed are a practical starting point; for drilling, 20–35 m/min and 0.10–0.25 mm/rev with pecking to clear chips. Flood coolant is recommended for deep holes and for any operation that generates fine dust.

Because H59 contains no deliberate lead, it does not break chips as cleanly as H59-1. Interrupted feed, chip breakers and high-pressure coolant solve most problems. Do not compensate for long chips by increasing feed beyond the tool’s capacity; that raises cutting temperature and can smear the bore. For deep small holes, drill in steps, retract fully and clear chips with air or coolant.

Threading and tapping are common operations on H59. Rolled threads are stronger than cut threads because the grain flows with the thread profile and no material is removed. Cut threads are acceptable for low-load fittings, but the thread flanks should be inspected for tearing. When tapping, use a spiral-flute tap for through holes and a spiral-point tap for blind holes, and keep the lubricant clean; brass chips recirculating in a blind hole are the usual cause of broken taps.

Plating and polishing are straightforward, but residue matters. H59 responds well to nickel and chrome plating after mechanical polishing and proper degreasing. Polishing compounds must be washed out of blind recesses before plating, or the bath will be contaminated and the deposit will blister. For decorative lacquer, a thin chemical conversion layer improves adhesion; skipping it produces peeling at sharp edges.

Selection Rules for Buyers

  • Choose H59 when you need a balance of strength, cost and machinability in a dry or lightly damp indoor part, and when the part will be polished, plated or brazed.
  • Choose H59-1 only when high-speed automatic machining is the dominant cost and potable water or food contact is not involved.
  • Choose H62 or H65 when the part must be cold formed deeply, soldered, or exposed to moving water; the higher copper content improves ductility and corrosion resistance.
  • Choose a bronze or DZR brass when the part sees chlorinated water, seawater or dezincification risk; plain H59 is not a dezincification-resistant alloy.
  • Specify temper by service: extruded for general machining, drawn and stress-relieved for long slender parts, hard drawn only where wear resistance matters more than ductility.

Diameter selection is not only a strength question. A 10 mm bar turned down to 6 mm loses most of its cold-work strength in the turned zone unless the part is re-annealed. If the drawing requires a hard outer skin, machine only the ends and keep the as-supplied surface where possible. For long shafts, specify straightness in the finished condition, not only in the bundle, and state whether the bar will be centreless ground after machining.

Environment is the other filter. H59 is adequate for indoor hardware, oil-filled enclosures and dry compressed air. It is marginal in continuous condensation and unsuitable in seawater or in water with free chlorine. Where a brass part must survive those conditions, use a higher-copper grade or a dezincification-resistant brass, and avoid direct coupling to stainless steel in a wet joint without an insulating sleeve.

Installation and Assembly Rules

H59 is usually joined by threading, brazing or mechanical fastening rather than by fusion welding. Fusion welding is possible but difficult: zinc boils at a low temperature, the arc is unstable and the fume is unpleasant. If welding is unavoidable, use a copper-based filler with a low zinc content, keep the heat input low, pre-clean the joint and provide local extraction. Do not weld a pressure-retaining H59 fitting unless the procedure has been qualified.

For threaded assemblies, tighten to a torque appropriate to the thread and the wall thickness, not to a generic steel value. Brass threads gall easily when dry; a compatible lubricant or a thread sealant reduces friction and improves sealing. Avoid over-tightening tapered threads, which can split a thin-wall fitting. When H59 is coupled to steel, galvanic corrosion attacks the steel at the joint if water is present; use an insulating washer or a dielectric union, and keep the brass area small relative to the steel area where possible.

For brazing, use a silver-based filler and a fluoride flux, heat the joint evenly and avoid overheating the bar beyond a dull red. Overheating coarsens the grain and can cause zinc loss at the surface, leaving a porous layer that will not take a polish. After brazing, wash the flux residue thoroughly; residual flux is hygroscopic and will corrode the joint in storage.

Common Misconceptions

  • “H59 means 59 HB hardness.” No. The number is the nominal copper content. Hardness depends on temper and bar size.
  • “H59 and H59-1 are interchangeable.” No. H59-1 is deliberately leaded for free machining; H59 is not. They differ in machinability, weldability and potable-water acceptability.
  • “All brass bars are corrosion-proof.” No. Plain brass dezincifies in chlorinated or marine water; H59 is an indoor alloy.
  • “A bigger diameter always gives a stronger thread.” Not if the thread is cut deeply into a thin wall; the thread root, not the nominal diameter, controls the load.
  • “Bright bar means peeled bar.” No. Bright can be chemical, turned or drawn. Specify the process if surface integrity matters.

Inspection and Acceptance

A practical receiving inspection for H59 bar covers four items: grade verification by spectrography or mill certificate, dimensions and straightness, surface condition, and mechanical properties where the part is safety-related. Spectrography is the only reliable way to separate H59 from H59-1 or from a scrap-derived alloy with high iron. Check diameter at three positions along the length and at 90° to each other; check straightness on a surface plate with a dial indicator; and inspect the ends for seams or laps that could propagate into a machined part.

For plated or polished parts, add a sample polish before mass production. A short run through the actual polishing sequence will reveal seams, porosity and inclusions that a visual check of the raw bar cannot. If the part is threaded, cut a test thread in the actual bar and inspect the flanks at 10× before releasing the lot.

Frequently Asked Questions

Is H59 suitable for drinking-water fittings?

Generally no. Plain H59 is not a dezincification-resistant grade and its lead is only residual, but it is still not the alloy to specify for potable water. Use a recognised DZR brass or a lead-free grade with the appropriate water-contact approval.

Can H59 be welded?

It can be brazed and soldered readily. Fusion welding is possible but needs a qualified procedure, low heat input, copper-based filler and good extraction because of zinc fume. For pressure parts, brazing or threaded assembly is preferred.

Why do my H59 bars bow after machining?

Residual stress from cold drawing is being released as material is removed. Specify stress-relieved bar, or rough machine, stress-relieve and finish machine in a second operation.

What is the difference between H59 and H62?

H62 has 60.5–63.5% copper, better cold ductility and better corrosion resistance in water; H59 is stronger and cheaper but less ductile and less resistant. H62 is preferred for deep drawing and plumbing, H59 for machined mechanical parts.

Which temper should I order for screw-machine parts?

For high-speed machining, H59-1 in drawn condition is usually the better choice. If H59 is required for metallurgical or regulatory reasons, order drawn and stress-relieved bar and adjust feeds, tooling and chip control.

What diameter tolerance is realistic?

h9 is a normal commercial tolerance for drawn bar; h11 is cheaper and adequate for many turned parts. Tighter than h9 should be justified by the finished part, because the bar will usually be machined anyway.

Need H59 brass bar, cut to length and with a mill certificate?

Request a Quotation

QIDAMT supplies copper and copper-alloy mill products from Liaocheng, with grade verification and export packing. Send drawing, diameter, temper and quantity for a quotation.