A 7075 aluminium plate is a high-strength aluminium-zinc-magnesium-copper alloy supplied in T6 or T651 temper for aerospace structures, 注塑模具, 工装, precision machinery and high-load components. It is the strongest common aluminium plate grade, and it is also the least forgiving: it is not weldable, it has poor corrosion resistance without protection, and it moves during machining unless the residual stress has been relieved.

什么 7075 Plate Is and Where It Is Used

7075 is an Al-Zn-Mg-Cu alloy standardised as AA7075, EN AW-7075 and UNS A97075. The zinc and magnesium additions, combined with copper and a small chromium addition, produce a very high strength after solution treatment and artificial aging. It is not a general fabrication alloy like 6061. It is selected when the part must carry high load with low weight, or when a mold or tool must resist deflection and wear.

Typical uses include aircraft wing and fuselage components, spar caps, landing gear parts, missile and space structures, 注塑模具, 吹塑模具, die-casting tools, 夹具和固定装置, precision machine parts, high-end bicycle frames and components, climbing hardware, robotics and defense equipment. In many of these applications the plate is machined from solid, and the amount of metal removed can be large.

7075 is not recommended for welded structures. The alloy is generally considered non-weldable by arc processes because the zinc-rich grain boundaries can crack during solidification and the heat-affected zone loses strength. If a design requires welding, 6061-T6或 5083 is usually the better choice. A 7075 part should be bolted, riveted, bonded or machined as one piece.

7075 铝板
A thick 7075 aluminium plate with a mill finish, stacked on a timber pallet and ready for sawing or machining.

牌号名称和化学成分

The certificate should report the alloy, 脾气, heat number and the results of the mechanical tests. The word 7075 还不够, because T6 and T651 have different residual stress states even when the chemistry is identical. A plate ordered as T6 may machine differently from the same plate ordered as T651, and the difference can be several millimetres of movement on a large part.

元素 7075 范围 (%) 角色 采购支票
和 0.40 最大限度 杂质 High silicon reduces toughness
铁 0.50 最大限度 杂质 Iron forms coarse phases
铜 1.20-2.00 Strength and age hardening 以下 1.2 loses strength
锰 0.30 最大限度 Impurity and grain control Excess manganese affects quench
镁 2.10-2.90 主要强化元素 Low magnesium lowers strength
铬 0.18-0.28 Grain boundary and stress corrosion Too little chromium hurts SCC resistance
锌 5.10-6.10 主要强化元素 High zinc increases cracking risk
的 0.20 最大限度 晶粒细化 Excess titanium affects casting
其他的 0.05 最大每个, 0.15 max total 残差 检查证书

Typical AA7075 / EN AW-7075 window. Confirm the exact standard and temper on the mill certificate.

Zinc and magnesium are the strengthening pair. During solution treatment they dissolve into the aluminium matrix; during aging they precipitate as fine particles that block dislocation movement. Copper adds strength and helps the aging response, while chromium improves resistance to stress corrosion cracking. A heat that is at the low end of the zinc and magnesium ranges may still meet the minimum tensile requirement, but it will have less margin in a highly loaded part.

Iron and silicon are impurities that form coarse intermetallic particles. These particles can act as crack initiation sites, especially in fatigue. A 7075 plate for an aerospace or fatigue-critical part should have iron and silicon at the low end of the range, not merely below the maximum. The certificate gives the numbers; a buyer who only checks the tensile result is missing half the story.

机械性能

7075-T6 is the standard high-strength temper. T651 is the same alloy and temper, but the plate is stretched after quenching to relieve residual stress. The tensile properties are essentially the same; the difference is dimensional stability during machining. For a thin sheet, T6 may be adequate. For a thick plate that will be machined into a large mold or fixture, T651 is usually the correct choice.

财产 7075-T6 / T651 typical 健康)状况 设计说明
抗拉强度, 室 572 兆帕 室温 Minimum values depend on thickness
屈服强度, RP0.2 503 兆帕 室温 高强度, low elongation
伸长, A50 11% 室温 低于 6061; avoid sharp notches
硬度 关于 150 HB 布氏硬度 Harder than 6061-T6
剪切强度 关于 331 兆帕 典型的 Useful for bolted joints
密度 2.81 克/立方厘米 标称 Lightweight compared with steel
弹性模量 71.7 GPa 标称 Lower stiffness than steel
导热系数 关于 120-130 瓦/米·K 20 摄氏度 Heat builds up in dry machining
Solution treatment 465-490 摄氏度 Mill process Not a shop heat treatment
Aging 关于 120 degrees C for 24 小时 Mill process T6 and T651 differ by stress relief

Typical room-temperature values for 7075-T6/T651 plate. Actual minima vary with thickness and standard; use the certificate and the applicable design code.

The combination of high strength and low elongation is what makes 7075 less forgiving than 6061. A sharp internal corner, a deep scratch or a tool mark can become a stress concentration and a crack starter. Design the part with generous fillets, remove tool marks, and do not use 7075 for a part that will be repeatedly bent or hammered. It is a strength alloy, not a toughness alloy.

Thermal conductivity is moderate for aluminium, but the high strength means cutting forces and heat can be significant. In dry machining, heat concentrates at the tool edge and can cause built-up edge or surface cracking. Use sharp tools, positive rake, adequate coolant and a rigid setup. A 7075 part that is machined with a dull tool may pass dimensional inspection and then fail in service because of subsurface damage.

7075 aluminium plate storage
7075 aluminium plates stored on edge in a warehouse, with the thick sections kept separate from thin sheet.

方面, 公差和板材数据

7075 plate is normally ordered by thickness, 宽度, length and temper. Thickness is the first variable because the strength and the amount of machining stock depend on it. 一个盘子就是 1 mm under nominal may still meet the standard tolerance, but the finished part may be undersize after cleanup. If the design has a minimum finished thickness, add the machining allowance and specify the minimum actual plate thickness.

范围 常用范围 典型公差 What to write on the order
厚度 6-150 毫米 ±0.3 to ±1.5 mm 标称, standard and minimum actual
宽度 1000-2500 毫米 0 到 +10 毫米 Finished width after sawing
长度 2000-6000 毫米 ±10毫米 Cut-to-length or mill length
平整度 — 关于 3-5 毫米每米 Critical for large molds
外倾角 — 关于 5 毫米以上 3 米 Check before machining
脾气 T6或T651 根据标准 T651 for thick machined parts
边缘 Sawed or milled Burr and squareness to agree Milled edge for a clean setup
表面 铣削加工 No cracks or deep scratches Inspect before machining
超声波测试 选修的 Per ASTM B594 For aerospace or critical parts

Typical commercial data for 7075 盘子. Tolerances vary by thickness, width and mill; 采购订单应注明标准和测量的可接受限度.

Flatness is not a cosmetic requirement for 7075. A plate that is bowed before machining will often distort further when the surface is removed, because the residual stress balance changes. T651 reduces this risk, 但这并不能消除它. If the part is large and thin, plan the machining sequence to remove material from both sides and to support the part evenly. Do not clamp a bowed plate flat and expect it to stay flat after the clamps are released.

Edge condition matters for safety and for machining. A sawed edge can have a burr that cuts gloves or interferes with setup. A milled edge gives a clean reference surface for indicating the part. For a plate that will be machined on both sides, specify a milled edge and a square corner if the setup depends on it. A plate with a ragged edge can slip in the vise and ruin the part.

如何 7075 Plate Is Made

The process starts with a direct-chill cast ingot. The ingot is homogenised at about 465 到 480 degrees C to dissolve the zinc- and copper-rich phases and reduce segregation. It is then hot rolled to plate thickness, solution treated at about 465 到 490 摄氏度, quenched and aged at about 120 degrees C for 24 小时. The quench must be fast enough to prevent coarse precipitation, but not so fast that the plate cracks.

T651 plate is stretched after quenching, typically by about 1.5 到 3%, to relieve residual stress. The stretch is a controlled permanent elongation that redistributes the internal stress. It is not a straightening operation in the ordinary sense; it is a metallurgical stress relief. A plate that is merely flattened after quenching may look straight but still move when machined.

The most common defects are residual stress, quench cracks, surface scratches, 边缘裂纹, thickness variation and flatness problems. Residual stress shows up as movement during machining, not as a visible defect at delivery. Quench cracks appear at the edges or in thick sections and are a reject. Surface scratches can be removed if they are shallow, but a deep scratch on a high-strength plate can become a fatigue crack starter.

A good mill records the ingot heat number, the solution treatment temperature, the quench delay, the aging cycle and the stretch percentage. The buyer does not need every parameter, but the certificate should connect the plate to a heat number and to the mechanical results. For aerospace or defense work, the traceability requirement is much stricter and may include ultrasonic inspection and a full heat-lot record.

机械加工和制造规则

The first rule is to use T651 for thick machined parts. T6 plate is cheaper and may be adequate for thin parts or parts with symmetrical material removal, but a large mold or fixture machined from T6 can distort by several millimetres. The cost difference is small compared with the cost of scrapping a mold.

The second rule is to plan the machining sequence. Remove material evenly from both sides, keep the part supported, and avoid heavy interrupted cuts that generate heat and vibration. 粗机, stress-relieve if the specification allows, then finish machine. For a large part, a intermediate stress relief can be the difference between a flat mold and a twisted one.

The third rule is tooling. 使用锋利的, coated carbide tools with positive rake and adequate clearance. Keep the tool path smooth; dwell marks and chatter leave stress concentrations. Use coolant or a minimum-quantity lubrication system that actually reaches the cut. Do not let chips recut; they damage the surface and raise the temperature. A 7075 part that is machined dry with a dull tool may look fine and fail later.

  • Order T651 for thick plates that will be machined on both sides.
  • Allow machining stock on all surfaces; do not design to the nominal plate thickness.
  • 粗机, stress-relieve if permitted, then finish machine.
  • Use sharp tools, positive rake and adequate coolant.
  • 避免尖锐的内角; use generous fillets.
  • 请勿焊接 7075; redesign for 6061 或者 5083 如果需要焊接.
  • Protect the surface from scratches and tool marks before and after machining.
  • Apply a corrosion protection system if the part will be exposed.

Common Mistakes Buyers and Engineers Make

错误 Why it goes wrong 更好的实践
Ordering T6 for a large mold Residual stress causes distortion during machining Use T651 for thick machined parts
Trying to weld 7075 Hot cracking and loss of strength Use 6061-T6 or 5083 for welded parts
使用 7075 in a marine environment Poor corrosion resistance without protection 使用 5083 或者 6061 有保护
Designing sharp internal corners Stress concentration and fatigue cracks Use generous fillets and smooth transitions
Machining with a dull tool Subsurface damage and heat Use sharp tools and coolant
假设 7075 is tougher than 6061 Lower elongation and notch sensitivity 使用 6061 where impact or bending dominates
Ignoring the protective film until late Scratches and contamination Keep the film on until the part is ready
Buying by alloy name only Temper and thickness may be wrong State alloy, 脾气, thickness and standard

Most 7075 failures come from using a high-strength alloy where a tougher or more corrosion-resistant alloy belongs, or from ignoring residual stress.

A frequent engineering mistake is to specify 7075 because it has the highest tensile strength, without checking the fatigue and corrosion requirements. In a cyclic load or a salty environment, a lower-strength alloy with better toughness and corrosion resistance may last longer. Strength is only one design property. The part that survives is the one that matches the failure mode, not the one with the highest data sheet number.

检查验收

Receiving inspection should start with the certificate and the plate label. Check the alloy, 脾气, 热数, 厚度, 宽度和长度. Measure thickness at several points and check flatness on a flat bed. Inspect the surface for scratches, cracks, dents and corrosion. For a thick plate, review the ultrasonic test report if the application is critical.

After machining, inspect the part for distortion, surface finish and dimensional accuracy. A plate that moved during machining may still be within tolerance if the finish pass was light, but the residual stress remains and the part may move again in service. If the part is a mold or a precision fixture, check it after a relaxation period, not only immediately after the last cut.

  • Match the alloy and temper on the label to the certificate.
  • 测量头部厚度, 中部和尾部, 和三个宽度.
  • Check flatness and camber before machining.
  • 检查两面是否有划痕, cracks and corrosion.
  • Review the ultrasonic report for thick or critical plate.
  • Record the heat number and plate identity for traceability.
  • Check the finished part after a relaxation period.
  • Keep a sample and the certificate for failure analysis.

常问问题

What is the difference between 7075-T6 and T651?

Both have the same alloy and aging treatment. T651 is stretched after quenching to relieve residual stress, which makes it more dimensionally stable during machining. Use T651 for thick machined parts.

能 7075 被焊接?

一般没有. Arc welding of 7075 is not recommended because of hot cracking and loss of strength in the heat-affected zone. Use 6061-T6 or 5083 如果需要焊接.

是 7075 强于 6061?

是的, considerably. 7075-T6 has about 572 MPa tensile strength versus about 310 MPa for 6061-T6. It is also less ductile and less corrosion resistant.

是 7075 suitable for marine use?

Not in direct seawater exposure without a protective coating. It has poor corrosion resistance compared with 5083 或者 6061. 使用 5083 for marine structures.

为什么会 7075 distort during machining?

Residual stress from quenching and rolling is released as material is removed. T651 reduces the stress, and a balanced machining sequence reduces the movement further.

能 7075 被阳极氧化?

是的, but the coating is less uniform and less protective than on 6061. Type II or Type III anodising can be used, and a sealed coating improves corrosion resistance.

What is the maximum service temperature of 7075?

The alloy is not intended for elevated temperature. Strength falls above about 100-150 摄氏度, and prolonged exposure above the aging temperature can overage the material.

多少钱一个 7075 plate weigh?

The density is about 2.81 克/立方厘米. A 1 m x 1 m plate at 20 毫米重约 56 千克. Use the actual thickness for freight and handling.

能 7075 be used for injection molds?

是的, especially for large molds where high strength and good thermal conductivity are needed. T651 is preferred for thick mold blocks, and the mold should be protected against corrosion.

What is the lead time for 7075 盘子?

Stock sizes may ship in days; custom thickness, width or ultrasonic testing may take several weeks. Send the full specification for a firm date.

是 7075 食品安全?

It is not typically used for direct food contact. If it is, the surface finish, coating and applicable food-contact standard must be checked.

Need a 7075 aluminium plate in T651 with a stated thickness and flatness?

索取报价

启达美特用品 7075 aluminium plate from Liaocheng. 发送厚度, 宽度, 长度, 脾气, flatness and destination for a quotation. 发送电子邮件至 sales@qidamt.com 或致电 +86 139 6951 8618 工作时间内 (格林威治标准时间+8).