7075 알루미늄 판: T651 Stress Relief, Machining and Aerospace Use

7075 알루미늄 판: <span class ="tr_" id="tr_6" data-source="" data-srclang="en" data-orig="T651 Stress Relief">T651 Stress Relief</span>, <span class ="tr_" id="tr_7" data-source="" data-srclang="en" data-orig="Machining and Aerospace Use">Machining and Aerospace Use</span>

ㅏ 7075 aluminium plate is a high-strength aluminium-zinc-magnesium-copper alloy supplied in T6 or T651 temper for aerospace structures, injection molds, tooling, precision machinery and high-load components. It is the strongest common aluminium plate grade, and it is also the least forgiving: it is not weldable, it has poor corrosion resistance without protection, and it moves during machining unless the residual stress has been relieved.

무엇 7075 Plate Is and Where It Is Used

7075 is an Al-Zn-Mg-Cu alloy standardised as AA7075, EN AW-7075 and UNS A97075. The zinc and magnesium additions, combined with copper and a small chromium addition, produce a very high strength after solution treatment and artificial aging. It is not a general fabrication alloy like 6061. It is selected when the part must carry high load with low weight, or when a mold or tool must resist deflection and wear.

Typical uses include aircraft wing and fuselage components, spar caps, landing gear parts, missile and space structures, injection molds, blow molds, die-casting tools, 지그 및 설비, precision machine parts, high-end bicycle frames and components, climbing hardware, robotics and defense equipment. In many of these applications the plate is machined from solid, and the amount of metal removed can be large.

7075 is not recommended for welded structures. The alloy is generally considered non-weldable by arc processes because the zinc-rich grain boundaries can crack during solidification and the heat-affected zone loses strength. If a design requires welding, 6061-T6 또는 5083 is usually the better choice. ㅏ 7075 part should be bolted, riveted, bonded or machined as one piece.

7075 aluminium plate
A thick 7075 aluminium plate with a mill finish, stacked on a timber pallet and ready for sawing or machining.

등급 지정 및 화학 성분

The certificate should report the alloy, 성질, heat number and the results of the mechanical tests. The word 7075 충분하지 않다, because T6 and T651 have different residual stress states even when the chemistry is identical. A plate ordered as T6 may machine differently from the same plate ordered as T651, and the difference can be several millimetres of movement on a large part.

요소 7075 범위 (%) 역할 Purchasing check
그리고 0.40 최대 불결 High silicon reduces toughness
철 0.50 최대 불결 Iron forms coarse phases
구리 1.20-2.00 Strength and age hardening 아래에 1.2 loses strength
망 0.30 최대 Impurity and grain control Excess manganese affects quench
마그네슘 2.10-2.90 주요 강화 요소 Low magnesium lowers strength
Cr 0.18-0.28 Grain boundary and stress corrosion Too little chromium hurts SCC resistance
아연 5.10-6.10 주요 강화 요소 High zinc increases cracking risk
의 0.20 최대 곡물 정제 Excess titanium affects casting
기타 0.05 각각 최대, 0.15 max total 잔차 Check the certificate

Typical AA7075 / EN AW-7075 window. Confirm the exact standard and temper on the mill certificate.

Zinc and magnesium are the strengthening pair. During solution treatment they dissolve into the aluminium matrix; during aging they precipitate as fine particles that block dislocation movement. Copper adds strength and helps the aging response, while chromium improves resistance to stress corrosion cracking. A heat that is at the low end of the zinc and magnesium ranges may still meet the minimum tensile requirement, but it will have less margin in a highly loaded part.

Iron and silicon are impurities that form coarse intermetallic particles. These particles can act as crack initiation sites, especially in fatigue. ㅏ 7075 plate for an aerospace or fatigue-critical part should have iron and silicon at the low end of the range, not merely below the maximum. The certificate gives the numbers; a buyer who only checks the tensile result is missing half the story.

기계적 성질

7075-T6 is the standard high-strength temper. T651 is the same alloy and temper, but the plate is stretched after quenching to relieve residual stress. The tensile properties are essentially the same; the difference is dimensional stability during machining. For a thin sheet, T6 may be adequate. For a thick plate that will be machined into a large mold or fixture, T651 is usually the correct choice.

재산 7075-T6 / T651 typical 상태 디자인 노트
인장강도, Rm 572 MPa 실내 온도 Minimum values depend on thickness
항복 강도, Rp0.2 503 MPa 실내 온도 고강도, low elongation
연장, A50 11% 실내 온도 보다 낮음 6061; avoid sharp notches
경도 에 대한 150 HB 브리넬 Harder than 6061-T6
Shear strength 에 대한 331 MPa 전형적인 Useful for bolted joints
밀도 2.81 g/cm3 명사 같은 Lightweight compared with steel
탄성률 71.7 평점 명사 같은 Lower stiffness than steel
열전도율 에 대한 120-130 W/m.K 20 degrees C Heat builds up in dry machining
Solution treatment 465-490 degrees C Mill process Not a shop heat treatment
Aging 에 대한 120 degrees C for 24 시간 Mill process T6 and T651 differ by stress relief

Typical room-temperature values for 7075-T6/T651 plate. Actual minima vary with thickness and standard; use the certificate and the applicable design code.

The combination of high strength and low elongation is what makes 7075 less forgiving than 6061. A sharp internal corner, a deep scratch or a tool mark can become a stress concentration and a crack starter. Design the part with generous fillets, remove tool marks, and do not use 7075 for a part that will be repeatedly bent or hammered. It is a strength alloy, not a toughness alloy.

Thermal conductivity is moderate for aluminium, but the high strength means cutting forces and heat can be significant. In dry machining, heat concentrates at the tool edge and can cause built-up edge or surface cracking. Use sharp tools, positive rake, adequate coolant and a rigid setup. ㅏ 7075 part that is machined with a dull tool may pass dimensional inspection and then fail in service because of subsurface damage.

7075 aluminium plate storage
7075 aluminium plates stored on edge in a warehouse, with the thick sections kept separate from thin sheet.

치수, Tolerances and Plate Data

7075 plate is normally ordered by thickness, 너비, length and temper. Thickness is the first variable because the strength and the amount of machining stock depend on it. 접시는 1 mm under nominal may still meet the standard tolerance, but the finished part may be undersize after cleanup. If the design has a minimum finished thickness, add the machining allowance and specify the minimum actual plate thickness.

매개변수 공통 범위 일반적인 공차 What to write on the order
두께 6-150 mm ±0.3 to ±1.5 mm 명사 같은, standard and minimum actual
너비 1000-2500 mm 0 에게 +10 mm Finished width after sawing
길이 2000-6000 mm ±10mm Cut-to-length or mill length
평탄 — 에 대한 3-5 미터당 mm Critical for large molds
캠버 — 에 대한 5 mm 이상 3 중 Check before machining
성질 T6 or T651 표준에 따라 T651 for thick machined parts
가장자리 Sawed or milled Burr and squareness to agree Milled edge for a clean setup
표면 밀 마무리 No cracks or deep scratches Inspect before machining
Ultrasonic test 선택 과목 Per ASTM B594 For aerospace or critical parts

Typical commercial data for 7075 그릇. Tolerances vary by thickness, width and mill; the purchase order should name the standard and the measured acceptance limits.

Flatness is not a cosmetic requirement for 7075. A plate that is bowed before machining will often distort further when the surface is removed, because the residual stress balance changes. T651 reduces this risk, but it does not eliminate it. If the part is large and thin, plan the machining sequence to remove material from both sides and to support the part evenly. Do not clamp a bowed plate flat and expect it to stay flat after the clamps are released.

Edge condition matters for safety and for machining. A sawed edge can have a burr that cuts gloves or interferes with setup. A milled edge gives a clean reference surface for indicating the part. For a plate that will be machined on both sides, specify a milled edge and a square corner if the setup depends on it. A plate with a ragged edge can slip in the vise and ruin the part.

How 7075 Plate Is Made

The process starts with a direct-chill cast ingot. The ingot is homogenised at about 465 에게 480 degrees C to dissolve the zinc- and copper-rich phases and reduce segregation. It is then hot rolled to plate thickness, solution treated at about 465 에게 490 degrees C, quenched and aged at about 120 degrees C for 24 시간. The quench must be fast enough to prevent coarse precipitation, but not so fast that the plate cracks.

T651 plate is stretched after quenching, typically by about 1.5 에게 3%, to relieve residual stress. The stretch is a controlled permanent elongation that redistributes the internal stress. It is not a straightening operation in the ordinary sense; it is a metallurgical stress relief. A plate that is merely flattened after quenching may look straight but still move when machined.

The most common defects are residual stress, quench cracks, surface scratches, 가장자리 균열, thickness variation and flatness problems. Residual stress shows up as movement during machining, not as a visible defect at delivery. Quench cracks appear at the edges or in thick sections and are a reject. Surface scratches can be removed if they are shallow, but a deep scratch on a high-strength plate can become a fatigue crack starter.

A good mill records the ingot heat number, the solution treatment temperature, the quench delay, the aging cycle and the stretch percentage. The buyer does not need every parameter, but the certificate should connect the plate to a heat number and to the mechanical results. For aerospace or defense work, the traceability requirement is much stricter and may include ultrasonic inspection and a full heat-lot record.

Machining and Fabrication Rules

The first rule is to use T651 for thick machined parts. T6 plate is cheaper and may be adequate for thin parts or parts with symmetrical material removal, but a large mold or fixture machined from T6 can distort by several millimetres. The cost difference is small compared with the cost of scrapping a mold.

The second rule is to plan the machining sequence. Remove material evenly from both sides, keep the part supported, and avoid heavy interrupted cuts that generate heat and vibration. 거친 기계, stress-relieve if the specification allows, then finish machine. For a large part, a intermediate stress relief can be the difference between a flat mold and a twisted one.

The third rule is tooling. 날카로운 것을 사용하라, coated carbide tools with positive rake and adequate clearance. Keep the tool path smooth; dwell marks and chatter leave stress concentrations. Use coolant or a minimum-quantity lubrication system that actually reaches the cut. Do not let chips recut; they damage the surface and raise the temperature. ㅏ 7075 part that is machined dry with a dull tool may look fine and fail later.

  • Order T651 for thick plates that will be machined on both sides.
  • Allow machining stock on all surfaces; do not design to the nominal plate thickness.
  • 거친 기계, stress-relieve if permitted, then finish machine.
  • Use sharp tools, positive rake and adequate coolant.
  • Avoid sharp internal corners; use generous fillets.
  • 용접하지 마십시오 7075; redesign for 6061 또는 5083 if welding is required.
  • Protect the surface from scratches and tool marks before and after machining.
  • Apply a corrosion protection system if the part will be exposed.

Common Mistakes Buyers and Engineers Make

Mistake Why it goes wrong Better practice
Ordering T6 for a large mold Residual stress causes distortion during machining Use T651 for thick machined parts
Trying to weld 7075 Hot cracking and loss of strength Use 6061-T6 or 5083 for welded parts
사용 7075 in a marine environment Poor corrosion resistance without protection 사용 5083 또는 6061 with protection
Designing sharp internal corners Stress concentration and fatigue cracks Use generous fillets and smooth transitions
Machining with a dull tool Subsurface damage and heat Use sharp tools and coolant
가정 7075 is tougher than 6061 Lower elongation and notch sensitivity 사용 6061 where impact or bending dominates
Ignoring the protective film until late Scratches and contamination Keep the film on until the part is ready
Buying by alloy name only Temper and thickness may be wrong State alloy, 성질, thickness and standard

Most 7075 failures come from using a high-strength alloy where a tougher or more corrosion-resistant alloy belongs, or from ignoring residual stress.

A frequent engineering mistake is to specify 7075 because it has the highest tensile strength, without checking the fatigue and corrosion requirements. In a cyclic load or a salty environment, a lower-strength alloy with better toughness and corrosion resistance may last longer. Strength is only one design property. The part that survives is the one that matches the failure mode, not the one with the highest data sheet number.

Inspection and Acceptance

Receiving inspection should start with the certificate and the plate label. Check the alloy, 성질, 열 번호, 두께, 너비와 길이. Measure thickness at several points and check flatness on a flat bed. Inspect the surface for scratches, cracks, dents and corrosion. For a thick plate, review the ultrasonic test report if the application is critical.

After machining, inspect the part for distortion, surface finish and dimensional accuracy. A plate that moved during machining may still be within tolerance if the finish pass was light, but the residual stress remains and the part may move again in service. If the part is a mold or a precision fixture, check it after a relaxation period, not only immediately after the last cut.

  • Match the alloy and temper on the label to the certificate.
  • Measure thickness at head, middle and tail, and at three widths.
  • Check flatness and camber before machining.
  • Inspect both faces for scratches, cracks and corrosion.
  • Review the ultrasonic report for thick or critical plate.
  • Record the heat number and plate identity for traceability.
  • Check the finished part after a relaxation period.
  • Keep a sample and the certificate for failure analysis.

자주하는 질문

What is the difference between 7075-T6 and T651?

Both have the same alloy and aging treatment. T651 is stretched after quenching to relieve residual stress, which makes it more dimensionally stable during machining. Use T651 for thick machined parts.

할 수 있다 7075 be welded?

Generally no. Arc welding of 7075 is not recommended because of hot cracking and loss of strength in the heat-affected zone. Use 6061-T6 or 5083 if welding is required.

~이다 7075 보다 강하다 6061?

예, considerably. 7075-T6 has about 572 MPa tensile strength versus about 310 MPa for 6061-T6. It is also less ductile and less corrosion resistant.

~이다 7075 suitable for marine use?

Not in direct seawater exposure without a protective coating. It has poor corrosion resistance compared with 5083 또는 6061. 사용 5083 for marine structures.

왜? 7075 distort during machining?

Residual stress from quenching and rolling is released as material is removed. T651 reduces the stress, and a balanced machining sequence reduces the movement further.

할 수 있다 7075 양극산화처리를 받다?

예, but the coating is less uniform and less protective than on 6061. Type II or Type III anodising can be used, and a sealed coating improves corrosion resistance.

What is the maximum service temperature of 7075?

The alloy is not intended for elevated temperature. Strength falls above about 100-150 degrees C, and prolonged exposure above the aging temperature can overage the material.

A는 얼마입니까? 7075 plate weigh?

The density is about 2.81 g/cm3. ㅏ 1 m x 1 m plate at 20 mm 무게는 약 56 kg. Use the actual thickness for freight and handling.

할 수 있다 7075 be used for injection molds?

예, especially for large molds where high strength and good thermal conductivity are needed. T651 is preferred for thick mold blocks, and the mold should be protected against corrosion.

What is the lead time for 7075 그릇?

Stock sizes may ship in days; custom thickness, width or ultrasonic testing may take several weeks. Send the full specification for a firm date.

~이다 7075 food safe?

It is not typically used for direct food contact. If it is, the surface finish, coating and applicable food-contact standard must be checked.

Need a 7075 aluminium plate in T651 with a stated thickness and flatness?

견적 요청

QIDAMT 용품 7075 aluminium plate from Liaocheng. 두께를 보내다, 너비, 길이, 성질, flatness and destination for a quotation. Email sales@qidamt.com or call +86 139 6951 8618 during working hours (GMT+8).