310S Stainless Steel Plate: Heat-Resistant Grade, Oxidation and Fabrication Guide
A 310S stainless steel plate is a high-nickel, high-chromium austenitic plate designed for service where ordinary 304 or 316L would scale, creep or collapse. It is the material behind furnace liners, kiln furniture, radiant tubes, exhaust shrouds and heat-treatment fixtures, and it is selected by thickness, kornstørrelse, flatness and elevated-temperature strength rather than by the word stainless alone.
What 310S Plate Is and Where It Is Used
310S is the low-carbon version of the 25% krom, 20% nickel heat-resistant austenitic family. The low carbon content does not make it stronger at room temperature; it makes it more tolerant of welding and high-temperature exposure by leaving less carbon available to form grain-boundary carbides. The grade is covered by UNS S31008, I 1.4845 and the Chinese designation 06Cr25Ni20, and it is normally supplied as hot rolled plate in the annealed and pickled condition.
The plate is used in equipment that spends its working life at 800 til 1150 degrees C in an oxidising atmosphere. Furnace shells, recuperator sections, radiant tube supports, annealing trays, kiln liners, incinerator baffles, exhaust manifolds, heat shields and thermal processing fixtures are typical. It also appears in the glass industry, ceramic firing furniture and some pyrometallurgical parts. In each case the common requirement is a stable oxide scale that does not spall off and expose fresh metal to further attack.
310S is not a general-purpose corrosion grade. It contains little molybdenum and is not designed for chloride pitting, seawater splash zones or wet process streams. A 310S plate that performs for years in a furnace can fail quickly in a coastal wash-down area, not because the plate is defective but because the application is outside the grade’s corrosion envelope. Buying by the name alone, without matching the environment, is the most common source of disappointment.

Karakterbetegnelse og kemisk sammensætning
The specification should name the standard and the heat number, not only 310S. A mill certificate for ASTM A240, I 10088-2 or GB/T 4237 gives the chemical analysis and the mechanical properties, while a delivery note that says 310S may not. The distinction matters because some suppliers sell 309S or a 25/20-type alloy with a composition outside the 310S window and expect the buyer to accept it as equivalent.
| Element | 310S range (%) | Fungere | Purchasing note |
|---|---|---|---|
| C | 0.08 max | Austenite stability; low carbon improves weld tolerance | Above 0.08 raises carbide precipitation risk |
| Og | 1.50 max | Oxidation resistance and deoxidation | High silicon can embrittle the scale |
| Mn | 2.00 max | Austenitisk tidligere | Not a substitute for nickel |
| P | 0.045 max | Residual impurity | High phosphorus reduces hot ductility |
| S | 0.030 max | Residual impurity | Sulphur hurts weld quality and scale adhesion |
| Cr | 24.0-26.0 | Oxide scale and hot corrosion resistance | Below 24% reduces scaling margin |
| I | 19.0-22.0 | Austenite stability and creep resistance | Low nickel allows sigma or ferrite |
| Fe | Balance | Matrix | Check residual elements on the certificate |
Typical 310S window. Confirm the exact standard and any customer restriction before releasing the heat.
Chromium and nickel work together at high temperature. Chromium forms the protective chromium oxide scale, while nickel stabilises the austenite so that the plate does not transform to a brittle phase during thermal cycling. A heat that sits at 24% krom og 19% nickel is still 310S, but it has less margin than one at 25.5% krom og 21% nikkel. That margin is what separates a furnace liner that survives ten campaigns from one that behaves well in the first month.
Carbon is deliberately kept at or below 0.08%. In a 25/20 austenitic steel, carbon can combine with chromium at grain boundaries during slow cooling or prolonged service, depleting the adjacent metal of chromium and creating a weak, corrosion-sensitive network. The low-carbon 310S grade reduces that risk, but it does not eliminate it. A plate that is held in the 600 til 900 degrees C range for thousands of hours can still form sigma phase or carbides, so the operating profile belongs in the selection discussion.
Mechanical and Thermal Properties
310S is an austenitic grade and is not hardenable by heat treatment. It is supplied annealed, with a fully austenitic structure and good ductility at room temperature. At elevated temperature the useful property is not the room-temperature yield strength but creep resistance and scale stability. Design values therefore need to come from the applicable high-temperature code, not from a room-temperature table copied from a catalogue.
| Ejendom | Typisk værdi | Condition or standard | Design note |
|---|---|---|---|
| Udbyttestyrke, Rp0.2 | 205 MPa minimum | Stuetemperatur, ASTM A240 | Do not use for hot-strength design |
| Trækstyrke, Rm | 515 MPa minimum | Stuetemperatur | Actual values often 550-650 MPa |
| Forlængelse, A50 | 40% minimum | Stuetemperatur | Low elongation suggests improper anneal |
| Hårdhed | 201 HB maximum | Brinell | Hardness is not a heat-resistance test |
| Tæthed | 7.98 g/cm3 | Nominal | Used for plate weight and freight |
| Termisk ekspansion | Om 17 x 10-6/K | 20-1000 degrees C | Allow roughly 17 mm pr meter |
| Termisk ledningsevne | Om 13-14 W/m.K | 20 degrees C | Lower than carbon steel |
| Continuous service | Up to about 1150 degrees C | Clean oxidising air | Reduce for cyclic or reducing service |
| Intermittent service | Up to about 1035 degrees C | Cyclic heating and cooling | Thermal shock shortens life |
Typical room-temperature and thermal data for annealed 310S. High-temperature allowable stress must be taken from the governing design code and the actual heat certificate.
The expansion figure is not a minor detail. A three-metre plate heated from 20 til 1000 degrees C grows by about 50 mm. If the plate is clamped between cold frames, the restraint can buckle it, crack the welds or pull the supports out of alignment. Expansion joints, slotted bolt holes and flexible anchors are not optional refinements; they are part of the way the material has to be used.
Thermal conductivity is low compared with carbon steel, so a 310S plate heats and cools more slowly and develops steeper through-thickness gradients during a fast cycle. That gradient drives distortion. A fabricator who treats the plate like mild steel and applies a local flame will create a permanent bow that cannot be removed by straightening. Controlled heating and cooling, with the part supported evenly, is part of the manufacturing method.

Dimensioner, Tolerances and Plate Data
310S plate is normally ordered by thickness, bredde, længde, surface and edge condition. Thickness is the first commercial variable, but flatness and camber are equally important for furnace panels and liners. A plate that is within thickness tolerance but bowed by 8 mm over a metre will fight the welder and leave gaps in a refractory-lined shell.
| Parameter | Common range | Typical tolerance or rule | What to state on the order |
|---|---|---|---|
| Tykkelse | 3-100 mm | Per ASTM A480 or EN 10029 | Nominal plus minimum actual |
| Bredde | 1000-3000 mm | Mill edge or trimmed | Finished width after trimming |
| Længde | 2000-12000 mm | Cut to length | Maximum lift and handling limit |
| Fladhed | — | Om 3 mm per metre typical | State if the plate is for a liner |
| Camber | — | Om 5 mm over 5 m typical | Critical for long panels |
| Edge | Sheared, plasma or machined | Burr and straightness to agree | Machined edge for visible or welded joints |
| Overflade | No.1 annealed and pickled | No scale, pits or embedded iron | Pickled and passivated if specified |
| Grain size | ASTM 4-8 typical | Per ASTM E112 | Coarse grain lowers ductility |
| Ultrasonic test | Valgfri | Per ASTM A578 | Required for pressure or critical parts |
Typical commercial ranges for 310S hot rolled plate. Tolerances vary with mill, width and thickness; the purchase order should name the standard and the measured acceptance limits.
Thickness tolerance is usually expressed as a minus and plus allowance, but the mill may roll to the plus side to meet a minimum weight. If the design has a minimum wall, put the minimum actual thickness on the order and ask for it to be certified. Do not accept a nominal thickness plus a verbal assurance. EN 0.5 mm shortfall on a 6 mm plate is an 8% loss of section, and at high temperature that lost section is exactly where creep damage begins.
Edge condition matters more on thick plate than on sheet. A sheared edge can carry a cold-worked rim and a burr; a plasma-cut edge can have a heat-affected zone and dross; a machined edge gives the cleanest joint preparation. For a furnace liner that will be welded edge to edge, specify a machined or edge-milled preparation with a defined bevel. For a plate that will be bolted, a sheared edge may be adequate if the burr is removed.
Flatness should be checked on a flat bed, not on the delivery truck. A plate that looks flat on a bed of soft timber may relax into a bow when it is lifted. Measure with a straight edge and a feeler gauge at several points, and record the result before cutting. If the plate is already bowed, stress-relieved cutting and welding may recover some of it, but a badly bowed plate should not be accepted for a visible liner.
How 310S Plate Is Made
The melt is produced in an electric arc furnace and refined in an argon-oxygen decarburisation vessel. The AOD step is important because it lowers carbon and controls nitrogen while protecting the high nickel and chromium content. The heat is then continuously cast into slabs, surface-ground and reheated for hot rolling. The rolling schedule must avoid excessive rolling temperature, which can produce a coarse grain and a poor surface, and avoid too low a finishing temperature, which can leave mixed grain and residual strain.
Efter rulning, the plate is annealed at about 1050 til 1150 degrees C and rapidly cooled to retain a fully austenitic structure. It is then pickled to remove scale and the chromium-depleted layer. Pickling of 25/20 steel is slower than pickling 304, and a mill that shortens the line to raise output can leave a smutty surface that looks acceptable under warehouse light but welds poorly. The surface should be uniform, grey to silver, with no dark patches or residual scale.
Fabrication starts with cutting. Plasma cutting is practical for thick plate, but the cut edge must be ground back to sound metal before welding because the plasma cut can leave a nitride-rich layer and dross. Waterjet cutting avoids the heat-affected zone but is slower and more expensive. Shearing is suitable for thinner plate and straight cuts, provided the blade and clearance are set for the thickness. Laser cutting of 310S is possible at moderate thickness but the oxide edge needs preparation.
Welding 310S requires a matching filler. Use ER310 or an equivalent 25/20 filler for 310S-to-310S joints. A 308L or 316L filler may produce a sound-looking weld at room temperature, but its high-temperature strength and scale resistance are lower, and the joint becomes the weak point in a furnace. Preheat is generally not required, but the plate should be dry and above dew point. Keep interpass temperature under about 150 degrees C, use a low heat input and avoid weaving that overheats the grain boundaries.
Post-weld cleaning matters. Remove all slag, heat tint and iron contamination. A nitric acid passivation or a pickling paste designed for high-alloy stainless restores the chromium oxide layer. Do not use carbon steel brushes, grinding wheels that have previously cut mild steel or contaminated blasting media. Embedded iron on a 310S plate becomes a rust spot in the first week, and the customer will blame the plate rather than the workshop.
Selection and Installation Rules
The first selection question is the actual atmosphere. 310S performs best in clean, oxidising air or combustion products with enough oxygen to maintain the scale. In a reducing atmosphere, in a vacuum, in a carburising atmosphere or in a gas stream with high sulphur and vanadium, the allowable temperature falls sharply and a different alloy may be needed. Do not approve 310S for a furnace just because the previous liner was 310S; check the fuel, the dew point and the contaminants.
The second question is the cycle. A continuous run at 1050 degrees C is less damaging than a daily cycle from ambient to 1050 degrees C, because thermal shock spalls scale and drives differential expansion. If the furnace cycles, reduce the peak metal temperature, slow the ramp and design supports that allow the plate to move. A thicker plate is not automatically better: it increases the through-thickness gradient and the thermal stress.
The third question is support and restraint. A 310S liner needs to be supported at intervals that limit sag at the operating temperature, but the supports must not lock the plate in both directions. Use sliding rails, slotted holes or flexible clips. Leave an expansion allowance of roughly 17 mm per metre between 20 og 1000 degrees C, and more if the plate runs hotter. At the cold end, do not weld a restraint that prevents growth; the restraint will either crack or buckle the plate.
- Confirm the atmosphere is oxidising and low in sulphur, vanadium and alkalis.
- State the peak metal temperature, the cycle frequency and the expected service life.
- Allow for thermal expansion in both length and width; use slotted or sliding supports.
- Select filler metal of the same 25/20 family, not 308L or 316L.
- Keep the plate dry before welding; moisture and carbon contamination cause porosity.
- Specify pickling or passivation after fabrication if the surface will be visible or cycled.
- Protect the plate from embedded iron during cutting, grinding and handling.
- Use ultrasonic inspection for thick pressure or safety-related plate.
Common Mistakes Buyers and Fabricators Make
| Mistake | What happens | Better practice |
|---|---|---|
| Buying 310S for chloride service | Pitting and crevice corrosion appear quickly | Use 316L, 904L or a duplex grade for chlorides |
| Using 308L or 316L filler | Weld scale fails before the parent plate | Use ER310 or a matching 25/20 fyldstof |
| Ignoring thermal expansion | Buckling, cracked welds or pulled supports | Design sliding joints and about 17 mm/m allowance |
| Treating the plate as mild steel during flame cutting | Hård, cracked edge and poor weld | Grind back the heat-affected zone before welding |
| Assuming thicker is always safer | Higher thermal gradient and more distortion | Use the design thickness and control the ramp |
| Welding with high heat input | Coarse grain and carbide precipitation | Low heat input, interpass below 150 C |
| Leaving scale or heat tint | Scale spalls and corrosion starts | Pickle and passivate after fabrication |
| Storing plates on damp ground | Edge rust and contamination | Store on dry timber, covered and ventilated |
Most failures are application or fabrication errors, not chemistry errors. A complete order description and a fabrication procedure prevent more problems than a higher grade.
One mistake deserves separate mention: using a 310S plate because it is available when the design actually needs a nickel-based alloy. På 1200 degrees C, in a reducing atmosphere or under severe thermal cycling, 310S is at the edge of its capability. A 310S plate may survive a trial run and then fail in production. If the operating conditions are outside the grade’s published envelope, do not let a successful short trial overrule the data.
Inspection and Acceptance
Acceptance starts with the certificate. Check the grade, varme nummer, standard, tykkelse, bredde, length and mechanical results. Confirm that the chemistry is inside the 310S window, especially chromium and nickel, and that carbon is at or below 0.08%. A certificate that reports only tensile strength is incomplete for a heat-resistant application.
Measure thickness at several points along the length and width, and check flatness and camber on a flat surface. Inspect both faces for scale, pickling smuts, rullemærker, scratches and embedded iron. A 310S plate often shows a faint rolling texture; that is normal. Mørk, raised scale or a rainbow heat tint is not normal and should be rejected or cleaned before fabrication.
- Match the heat number on the plate to the certificate.
- Verify chromium, nickel and carbon against the 310S range.
- Measure thickness at head, middle and tail, and at three widths.
- Check flatness, camber and edge burr on a flat bed.
- Inspect both surfaces for scale, gruber, cracks and iron contamination.
- For thick or critical plate, review the ultrasonic test report.
- Record the plate identity so it remains traceable after cutting.
- Keep a sample and the certificate for future failure analysis.
If the plate is for a pressure-retaining component, the acceptance plan should also include ultrasonic examination for internal discontinuities and a hardness or PMI check on the first cut piece. PMI is useful for confirming the chromium and nickel range, but a handheld X-ray gun may not separate 310S from 309S with confidence. Use a laboratory analysis or a certified reference method when the grade is critical.
FAQ
Hvad er forskellen mellem 310 and 310S?
310S has a lower carbon maximum, som regel 0.08% mod 0.25% for 310. The lower carbon improves weldability and reduces carbide precipitation, but it does not change the high-temperature strength class.
Can 310S be used at 1200 degrees C?
Only in a clean oxidising atmosphere and with a design that accounts for creep. The usual continuous limit is about 1150 degrees C, and cyclic service is lower. Above that, a nickel-based alloy or a ceramic may be required.
Is 310S magnetic?
Annealed 310S is austenitic and essentially non-magnetic. Cold work, welding or sigma formation can make it weakly magnetic. A strong magnet response is a reason to check the structure, not proof of a wrong grade.
Can 310S be welded with 316L filler?
It can produce a joint that looks sound, but the weld metal has lower high-temperature strength and scale resistance. Use a matching 25/20 filler such as ER310 for service at temperature.
Does 310S resist seawater?
Ingen. It has little molybdenum and is not a chloride-resistant grade. Use 316L, 904L or a duplex stainless steel for seawater and chloride-bearing process streams.
Why does a 310S plate distort after welding?
The plate has a low thermal conductivity and high expansion coefficient, so local heat creates a steep gradient. Low heat input, balanced welding, proper support and stress relief reduce distortion.
What surface finish should I order?
No.1 annealed and pickled is standard for hot rolled plate. If the surface will be visible or cycled, specify pickling and passivation after fabrication and ban iron contamination.
Can I get 310S plate cut to size?
Ja. Waterjet, plasma, laser and machined edge options are available. State the edge preparation and whether the heat-affected zone must be removed before welding.
How do I store 310S plate?
Keep it dry, flat and covered, on timber rather than concrete. Avoid contact with carbon steel, chlorides and damp insulation. Inspect the edges periodically for rust.
Is a mill certificate required?
For furnace, pressure, export or safety-related work, ja. The certificate should link the plate to a heat number and report chemistry and mechanical properties.
Need a 310S heat-resistant plate with a stated thickness, flatness and edge preparation?
QIDAMT supplies 310S stainless plate from Liaocheng. Send tykkelsen, bredde, længde, operating temperature, atmosphere and destination for a quotation. Email sales@qidamt.com or call +86 139 6951 8618 during working hours (GMT+8).
FREMSKRIDT