S350GD+Z Galvanized Steel Coil
Structural-grade zinc coated coil, 350 MPa 最小屈服强度, Z275 for frames and outdoor structures.
S350GD+Z is a hot-dip galvanized structural steel coil with a 350 MPa minimum yield strength. It lets a frame, purlin or panel carrier be designed at a thinner gauge than DX51D while keeping the corrosion protection of zinc. QIDAMT supplies S350GD+Z in 0.8–3.0 mm, Z100–Z350, slit to width and packed for export.
The grade is common in steel framing, 太阳能支架, 卡车车身, racking and agricultural structures. This page explains the mechanical limits, the coating options, how the higher strength changes forming and welding, and where the grade should not be used.
Where S350GD+Z Coil Is Used
- Light steel framing, 螺柱, joists and wall panels
- Solar mounting rails, brackets and ground-mount structures
- 卡车车身, trailer panels and refrigerated van liners
- Warehouse racking, shelving and mezzanine decking
- 农业大棚, livestock equipment and fencing
- HVAC support frames and equipment housings
The economic case is simple: 在 350 兆帕产量, A 1.5 mm section can replace a 2.0 mm DX51D section in many bending-dominated parts, saving weight and coating area. The case fails when stiffness, 不是力量, governs — a thinner gauge flexes more even if the stress is acceptable.
化学成分
| 元素 | 限制 (%) | 角色 |
|---|---|---|
| 碳 (C) | 0.20 最大限度 | Strength with weldability |
| 硅 (和) | 0.60 最大限度 | 力量; too high hurts coating |
| 锰 (锰) | 1.70 最大限度 | 主要强化元素 |
| 磷 (磷) | 0.10 最大限度 | Solid solution strengthening |
| 硫 (S) | 0.045 最大限度 | Inclusion control |
| 铝 (铝) | 0.015 分钟 | Fine grain and deoxidation |
| 铌 + 的 | 0.20 最大限度 | Micro-alloying for consistent yield |
The chemistry is designed to reach 350 MPa without the carbon level that would make welding difficult. That is why S350GD can be spot welded and roll formed on equipment used for thinner commercial grades, provided the gauge and current are adjusted.
机械性能
| 财产 | 要求 | 设计说明 |
|---|---|---|
| 屈服强度ReH | ≥350 MPa | Use the certified value, not the minimum |
| 拉伸强度Rm | 420 – 560 兆帕 | Check against connection design |
| 伸长率A80 | ≥16% | Enough for normal profiling, not deep drawing |
| 镀层质量 | Z100 – Z350 g/m² | Z275 standard for outdoor frames |
| 厚度 | 0.8 – 3.0 毫米 | 以下 0.8 mm forming limits tighten |
| 线圈ID | 508 / 610 毫米 | Confirm uncoiler capacity |
The tensile range is wide because mills balance strength against elongation. A coil at 540 MPa tensile will form differently from one at 430 兆帕; for roll-formed profiles, ask for a consistent heat and check the first coil before full production.
Coating and Surface Options
| 涂层 | 总质量 (克/平方米) | 典型曝光 |
|---|---|---|
| Z100 | 100 | 室内的, 干燥, 绘 |
| Z180 | 180 | 室外有遮蔽, 绘 |
| Z275 | 275 | 室外结构, 屋顶, 管道 |
| Z350 | 350 | Severe exposure, coastal or industrial |
For structural frames that will be painted, Z275 is the usual balance. For coastal sites or uncoated outdoor use, Z350 extends service life. Remember that the coating protects the steel only while it is continuous; 切边, drilled holes and weld zones need a zinc-rich repair coating.
成型, Roll Forming and Welding
S350GD work-hardens more than DX51D, so bending radii should be generous relative to thickness and the bend line should run across the coil width where possible. Springback is higher than commercial grades: a 90° bend may need over-bending of 2 – 4° depending on thickness and tooling.
Roll forming is the natural process for this grade. Set the rolls for the certified yield, keep the strip tension steady and avoid abrupt transitions that can crack the coating at the corners. For profiles with holes, punch before forming only if the distortion is acceptable; otherwise punch after forming.
焊接: spot welding is standard for thin gauges; for structural joints, use the procedure qualified for the actual thickness and remove zinc from the weld zone. Do not use S350GD as a substitute for a true structural plate in a welded load path without checking the welding procedure and heat input.
评选规则
- Match the gauge to the governing case: bending strength, deflection, or local buckling. Higher yield does not improve stiffness.
- Use Z275 as the default for outdoor frames; upgrade to Z350 only where the coating is exposed and unpainted.
- For roll-formed profiles, keep the same heat for a production run so springback does not drift.
- Do not deep draw S350GD; its elongation is adequate for profiling, not for drawing.
- If the part is painted after forming, specify skin-passed, oiled and chromate-free material and confirm paint compatibility.
常见错误
- Replacing 2.0 mm DX51D with 1.5 mm S350GD and assuming the panel will be as stiff.
- Ignoring springback because the grade is labelled structural.
- Cutting the coil with a dull blade and leaving a burr that rusts first.
- Welding through zinc without fume extraction.
- Mixing S350GD and DX51D parts in the same painted assembly without noting the different surface reactivity.
Corrosion Behaviour and Service Life
The zinc coating protects the steel at scratches, cut edges and fixing points — exactly where painted structural frames fail first. Service life therefore depends on coating mass, exposure category and detailing, not on the yield strength.
- Rural and indoor service: Z100 – Z180 is usually enough when the part is painted.
- 城市的, industrial and sheltered outdoor service: Z275 is the practical minimum.
- 沿海, de-icing salt or ammonia-rich livestock buildings: specify Z350 and inspect cut edges.
- Water traps, unvented box sections and contact with treated timber shorten life regardless of coating mass.
- Dissimilar metals in contact (铜, 黄铜, 防锈的) cause galvanic attack on the zinc; isolate with a suitable fastener or coating.
Tolerances and Inspection
| 物品 | Normal supply | Check before production |
|---|---|---|
| 厚度 | ±0.05 mm typical | Measure at three points across the width |
| 宽度 (狭缝) | ±0.5毫米 | Check both ends of the coil |
| 外倾角 | ≤ 5 毫米每 2 米 | Matters on long roll-formed profiles |
| 屈服强度 | ≥350 MPa certified | Compare certificate with trial coil |
| 镀层质量 | Z100 – Z350 | Weigh-strip or certificate |
| 表面 | Regular / skin-passed | Confirm for painted parts |
Where S350GD+Z Should Not Be Used
- Deep-drawn parts with sharp radii — use DX52D or DX53D instead.
- Heavy welded load paths that require a qualified structural plate procedure.
- Parts where deflection, not stress, governs the design; a thinner high-strength sheet will flex more.
- High-temperature service where zinc coating degrades or embrittles the steel.
Packing and Delivery
Coils are supplied eye-to-sky or eye-to-wall, 用钢带捆扎, edge-protected and wrapped. For container shipment, the coil weight and eye direction must be fixed before booking; a coil that is too large for the door cannot be loaded later. We supply mill certificates, coating mass records and pre-shipment photos.
常见问题解答
Is S350GD+Z a structural grade?
是的. 在 10346 defines S350GD with a minimum yield of 350 MPa for structural use. It is not a plate grade and should not be substituted for hot-rolled structural plate in heavy welded connections without engineering review.
What does the Z275 coating mean?
Z275 is a total zinc coating mass of 275 克/平方米, 关于 19 每边微米. It is the usual choice for outdoor structural parts and roofing.
Can S350GD be galvanized after welding?
The coil is already zinc coated. If the finished part is hot-dip galvanized after fabrication, tell us before ordering so the surface and venting can be planned; double coating is not a substitute for correct detailing.
Do you supply slit widths?
是的. Send finished width, tolerance and edge condition. Slitting is done from master coil with edge protection on the rewound coil.