H59 Brass Hexagonal Bar: Across-Flats Tolerance and Machining Guide
H59 brass hexagonal bar is a copper-zinc mill product supplied with six flat faces, so a wrench, socket or fixture can grip it without a secondary milling operation. The grade is chosen for moderate strength, good hot workability and a cost level below high-copper brasses, and the hexagon is chosen for nuts, valve bodies, threaded fittings and machine parts that must be driven or indexed from the outside.
What H59 Hexagonal Bar Is and Where It Is Used
H59 is a binary copper-zinc alloy with a nominal copper content of 57–60%. In the wrought condition it contains both alpha and beta phases, which gives it higher strength than single-phase 65/35 brass while keeping enough ductility for extrusion and cold drawing. The hexagonal shape is not a separate grade or a heat treatment; it is a rolled or drawn profile with six equal flats and six equal corners.
The form is used wherever a part must be turned from bar stock and then gripped by a standard wrench. Common examples include hex nuts, union bodies, valve bonnets, hose adapters, compression fittings, grease nipples, standoff spacers, terminal studs, instrument cases and small structural fasteners. In each case the hexagon performs two jobs: it provides a driving surface and it indexes the part in a fixture at 60-degree intervals.
H59 hex bar is also common in decorative and electrical hardware. Lamp holders, cable glands, switch shafts, earthing terminals and brass spacers are often machined from hex stock because the finished part needs a wrench flat and a polished or plated surface. The alloy takes nickel and chrome plating well, and it can be brazed or soldered without the cracking problems associated with leaded free-cutting brasses.
A buyer should separate three similar products before requesting a quotation. H59 round bar is turned from the solid and has no wrench flats. H59-1 hex bar is the leaded free-cutting variant, with deliberately added lead for high-speed automatic machining. H59 hex bar is the low-lead residual version, better for brazing, polishing and applications where leaded stock is restricted. The external shape may look identical, but the machining behaviour and the regulatory status are not.

Grade Designation and Chemical Composition
H59 is specified in China by GB/T 5231 for wrought copper alloys and sits close to the ISO CuZn40 family. The exact limits vary by product form and by mill practice, so the purchase order should name the standard, the temper and the dimensional class rather than only the grade letters. The table gives a typical window for hex bar; it is a purchasing guide, not a substitute for the mill certificate.
| unsur | Typical H59 range (%) | Function in the alloy | Purchasing note |
|---|---|---|---|
| Cu | 57.0–60.0 | Sets colour, conductivity and phase balance | Below 57% raises beta fraction and reduces ductility |
| Zn | Baki | Raises strength, lowers melting point | Zinc loss during melting is normal; check analysis |
| Pb | ≤ 0.50 | Residual impurity in H59 | H59-1 carries 0.8–1.9% Pb by design |
| Fe | ≤ 0.30 | Grain refinement and strength | Excess iron forms hard particles and dulls tools |
| Sn | ≤ 0.20 | Minor strength increase | Residual; not a substitute for tin bronze |
| Al | ≤ 0.10 | Deoxidation aid | Too much aluminium hurts hot ductility |
| Sb | ≤ 0.01 | Unintended impurity | Brittle antimonides above the limit |
| Bi | ≤ 0.002 | Unintended impurity | Causes hot-short cracking in drawing |
| P | ≤ 0.01 | Residual deoxidiser | Excess phosphorus embrittles the bar |
| Total impurities | ≤ 1.0 | Control of scrap-derived melts | Spectrography is the practical check |
Typical GB/T 5231 window for H59 wrought brass. Confirm the current edition and any customer-specific lead limit before releasing the order.
The copper level is the single most important number in the specification. At the low end of the range the alloy is stronger and harder, but it is also less ductile and more prone to cracking during cold drawing or severe bending. At the high end the bar is softer, easier to polish and more resistant to dezincification, but it costs more because copper is the expensive element. A mill that routinely runs near 58% copper will produce a different machining response from one that runs near 59.5%.
Sifat Mekanikal
Hex bar is normally supplied in the extruded condition, sometimes marked M or R, or in a cold-drawn and stress-relieved condition for automatic machining. Cold drawing raises tensile strength and hardness, lowers elongation and leaves residual stress that can bow a long part after material is removed. The values below are typical room-temperature ranges for 10–40 mm bar; they are design guidance rather than guaranteed minimums.
| Harta benda | Tersemperit (M) | Drawn and stress relieved | Drawn hard |
|---|---|---|---|
| 0.2% proof stress, Rp0.2 (MPa) | 170–235 | 220–300 | 310–410 |
| Kekuatan tegangan, Rm (MPa) | 390–490 | 450–560 | 550–690 |
| Pemanjangan, A (%) | 22–32 | 16–25 | 6–12 |
| Kekerasan, HB | 85–110 | 105–130 | 130–170 |
| Kekonduksian elektrik (% IACS) | 25–29 | 25–29 | 24–28 |
| Kekonduksian terma (W/m·K) | 90–110 | 90–110 | 85–105 |
Typical values for H59 hex bar at room temperature. Verify temper, test direction and sampling position on the mill report for safety-related parts.
Three practical consequences follow. Pertama, the same nominal grade can differ by 40% in proof stress depending on temper, so a drawing that specifies only H59 leaves the mechanical result to the mill. Kedua, cold-drawn hex bar is not stress-free: a long nut or valve body can distort after the bore is machined unless the bar was stress-relieved before cutting. Ketiga, H59 loses strength quickly above 200 °C and should not be used for hot steam or exhaust components without a proper high-temperature alloy.

Dimensi, Tolerances and Supply Forms
Hex bar is ordered by the distance across flats, not by the distance across corners. For a regular hexagon the across-corners dimension is 1.1547 times the across-flats dimension, so a 19 mm hex has a corner-to-corner distance of about 21.9 mm. The wrench size is the across-flats value. If a drawing gives only the circumscribed circle, convert it before ordering or the part will not fit the intended socket.
| Ciri | Common range | Toleransi tipikal | What to state on the order |
|---|---|---|---|
| Across flats | 5–70 mm | h9, h11 or ±0.10 mm | Nominal AF, tolerance class and wrench standard |
| Across corners | Derived | AF × 1.1547 | Check clearance in the socket or housing |
| Panjang | 1–6 m | +5 / 0 mm | Fixed length or random mill length |
| Kelurusan | — | 0.5–2 mm per metre | Critical for bar feeders and long shafts |
| Jejari sudut | — | 0.3–1.0 mm typical | Sharp corners chip and damage handling equipment |
| Twist | — | ≤ 1° per metre | Matters for long fixtures and guide rails |
| Permukaan | — | Terang, pickled or peeled | Peeled bar is preferred for plating |
| tamat | — | Saw cut, deburred or chamfered | Chamfer reduces thread start damage |
Typical commercial windows for drawn and extruded hex bar. Tolerances tighter than h9 should be justified by the finished part, because most hex stock is machined after delivery.
The tolerance that causes the most disputes is across flats. A bar at the low limit of h11 will rattle in a standard wrench, while a bar at the high limit may not enter a socket that was sized for the nominal dimension. For safety-critical nuts and valve bodies, specify the wrench standard and the acceptable torque, then check the finished part with a go/no-go gauge rather than trusting the bar certificate alone.
Length and straightness are usually treated as secondary, but they matter on automatic lathes and bar feeders. A bundle that is straight in storage can develop a bend after the first cut because residual stress is released. If the bar will run through a guide bush, specify straightness in the cut length and ask the mill to stress-relieve before straightening. For long hex shafts, specify twist as well; a twisted bar will not sit flat in a fixture even when the across-flats dimension is correct.
How H59 Hex Bar Is Made
The melt is prepared from cathode copper and zinc ingot in an induction furnace, with a charcoal or borax cover to reduce zinc loss. Phosphorus is added in a controlled amount as a deoxidiser, then the analysis is checked by spectrography before casting. The billet is homogenised to even out the copper distribution and to dissolve coarse intermetallics. Without that step, the extruded bar can show bands of hard phase that interrupt machining and dull tools.
Extrusion produces the hexagonal profile directly through a shaped die at 700–800 °C. The bar leaves the press with a fine-grained core and a thin oxide skin, then is straightened and cut. Smaller hex sizes are often cold drawn from round rod through a hex die; drawing improves the surface, tightens the across-flats tolerance and raises strength. Interpass annealing is required between heavy reductions, otherwise the bar cracks at the corners.
After the final pass the bar is straightened on a rotary or two-roll straightener, cut to length and finished as bright, peeled or pickled. Peeling removes the extrusion or drawing skin and exposes sound metal, which is the best starting condition for plating and polishing. Pickling is cheaper but can leave a smutty surface and can exaggerate shallow seams. A light stress-relief anneal at 250–350 °C is used for long parts that must hold straightness after machining.
The defects that most often reach the customer are corner cracks, longitudinal seams, residual twist and bar-to-bar colour variation. Corner cracks come from excessive reduction without annealing or from a die with a worn radius. Seams come from billet porosity or from a folded oxide layer during extrusion. Twist comes from poor straightener set-up. Colour variation is usually a function of pickling bath condition, not of grade, but it is often mistaken for a different alloy and should be resolved with a certificate and a spectrograph check.
Machining and Secondary Operations
H59 hex bar machines like a medium-strength brass. It is more ductile than H59-1, so chips tend to run long and stringy. Use sharp positive-rake carbide with a polished rake face, high surface speed and moderate feed. As a starting point for turning, 250–450 m/min at 0.08–0.20 mm/rev; for drilling, 20–35 m/min at 0.10–0.25 mm/rev with pecking. Flood coolant is advisable for deep holes and for any operation that produces fine dust.
The hexagon is a natural clamping feature, but it is also a weak point. Clamp on the flats with soft jaws or a collet, never on the corners, because point loading can crush the edge and create a stress riser. A six-jaw chuck distributes clamping force evenly; a three-jaw chuck on a hex bar contacts only three flats and tends to rotate the bar under heavy cuts. For second operations, use a hexagonal collet or a machined soft-jaw bore that matches the across-flats dimension.
Threading is usually the reason for choosing hex stock. Cut threads are acceptable for low-load fittings, but rolled threads are stronger because the grain flows along the thread profile and no material is removed. When cutting a thread, support the bar close to the die or tool and check coaxiality with the hexagon; an eccentric thread will make the nut sit crooked and will leak on a tapered fitting. For tapped holes, use a spiral-flute tap for through holes and a spiral-point tap for blind holes, and clear chips often.
Plating and polishing follow the usual brass sequence: mechanical polish, alkaline degrease, acid activation, nickel strike and final deposit. Polishing compound must be removed from blind holes and from the corners of the hexagon before plating, or the bath will be contaminated and the deposit will blister. For lacquer finishes, a thin conversion coating improves adhesion; without it, the coating peels first at the sharp corners.
Selection Rules for Buyers
- Select by across flats, not by diameter. The wrench, socket and fixture are sized by AF, and the corner dimension only matters for clearance.
- Choose H59 for brazed, polished or plated parts. Its low residual lead makes it more forgiving than H59-1 in joining and finishing.
- Choose H59-1 only for high-speed automatic machining. The added lead shortens chips, but it restricts potable-water and food-contact use.
- Choose H62 or H65 when the part will be deep drawn or exposed to moving water. Higher copper improves ductility and corrosion resistance.
- Specify temper and stress relief for long parts. A hard-drawn bar that is straight in the bundle may bow after the first machining cut.
- Avoid H59 in seawater and chlorinated water. Plain brass dezincifies; use a DZR grade or a copper alloy with a proven water approval.
The second selection question is surface finish. Bright drawn bar is adequate for general machining and gives a good starting surface for plating. Peeled bar costs more but removes seams and oxide, which is important for polished decorative parts and for pressure fittings. Pickled bar is the cheapest clean surface but can hide shallow defects; it should not be accepted for a part that will be pressure tested without a proof-machined sample.
Size selection should account for the thread and the wall thickness, not only the wrench. A nut that fits a 24 mm wrench may need a 24 mm AF bar, but the thread root and the wall around it determine whether the nut will strip. For a given thread, calculate the required wall thickness first, then choose the next larger standard hex size. Do not reduce the hex size to save material if the resulting wall is below the minimum for the thread and the service load.
Installation and Assembly Rules
H59 hex parts are usually joined by threads, brazing or mechanical fastening rather than by fusion welding. Brazing with a silver-based filler and a fluoride flux is the standard method for tube and fitting assemblies. Heat the joint evenly, keep the flame moving, and stop before the bar reaches a dull red. Overheating coarsens the grain, burns out zinc at the surface and leaves a porous layer that will not polish or plate.
For threaded assemblies, tighten to the torque appropriate to the thread and wall thickness, not to a generic steel value. Brass threads gall easily when dry; a compatible lubricant or thread sealant reduces friction and improves sealing. Tapered threads should not be over-tightened, because the wedge action can split a thin-wall fitting. When a brass part is coupled to steel in a wet joint, galvanic corrosion attacks the steel; use an insulating washer or a dielectric union and avoid a large cathodic area.
Hex parts that are driven with a wrench should be designed with a chamfer on the leading corner. A sharp corner chips during handling and can damage the plating at the edge. For parts that are repeatedly assembled, specify a radius or chamfer and a torque value in the drawing. If the part will be used as a jam nut, check that the hex faces are parallel and square to the thread; a skewed face concentrates load on one side and loosens under vibration.
Salah Tanggapan Biasa
- “H59 means 59 HB hardness.” The number is the nominal copper content, not a hardness or a tensile class.
- “A hex bar is stronger than a round bar of the same AF.” The hexagon removes material at the corners; strength depends on the actual cross-section and temper.
- “Across corners is the wrench size.” Wrenches are sized across flats. Across corners is only for clearance.
- “H59 and H59-1 are interchangeable.” H59-1 is deliberately leaded for free machining; H59 is not.
- “All brass hex bar is corrosion-proof.” Plain brass dezincifies in chlorinated or marine water.
- “Bright bar is always peeled bar.” Bright can be as-drawn, turned or chemically brightened; the processes leave very different surfaces.
Inspection and Acceptance
Receiving inspection for H59 hex bar should cover grade, dimensi, kelurusan, surface and, where the part is safety-related, sifat mekanikal. Spectrography is the only practical way to distinguish H59 from H59-1 or from a scrap-derived alloy with high iron. Check across flats at three positions along the length and at 60-degree intervals; check across corners only if the drawing requires it. Measure straightness on a surface plate with a dial indicator, and check twist by mounting the bar in V-blocks.
For a new supplier, ask for a sample length and machine a test part before releasing the lot. A short turning and threading trial will reveal seams, porosity, corner cracks and inconsistent machinability that a visual inspection cannot. If the part will be plated, include a sample polish and plate run; a blister or a dull patch at the corner is a sign of a subsurface defect, not a plating bath problem.
Soalan Lazim
What does H59 mean on a hex bar?
H59 is the Chinese wrought brass grade with a nominal copper content of 57–60%. The number refers to copper, not to hardness, tensile strength or a wrench size.
How do I convert across flats to across corners?
Multiply the across-flats dimension by 1.1547. A 19 mm AF hex has an across-corners distance of about 21.9 mm. Use the AF value for wrench and socket selection.
Is H59 hex bar free-cutting?
Not in the strict sense. H59-1 is the leaded free-cutting variant. H59 has only residual lead, so it machines well at moderate speeds but produces longer chips and needs good chip control.
Can H59 hex bar be welded?
Brazing and soldering are straightforward. Fusion welding is possible but needs a qualified procedure, low heat input and copper-based filler because zinc vaporises and the arc is unstable.
Why do hex nuts crack at the corners after threading?
The usual causes are a bar at the low end of the copper range, insufficient stress relief, or a die that removes too much wall at the corner. Check the bar certificate, the thread root and the chamfer.
What tolerance should I specify for a standard wrench?
h11 is adequate for many commercial nuts, h9 is better for production tooling and repeated assembly. Tighter than h9 is rarely needed because the part is usually machined after delivery.
Need H59 brass hex bar with a stated across-flats tolerance and mill certificate?
QIDAMT supplies copper and copper-alloy bar, pinggan, strip and tube from Liaocheng, with grade verification, cut-to-length service and export packing. Send the AF size, perangai, length and quantity for a quotation.
KEMAJUAN