DX52D+Z Galvanized Steel Coil – Drawing and Forming Quality - 진전

전화: +86-13969518618    이메일: sales@qidamt.com

에 대한 연락하다 |

GALVANIZED · EN 10346 DX52D+Z

DX52D+Z Galvanized Steel Coil

Drawing-quality zinc coated coil, 0.3–2.0 mm, Z100–Z275, 코일 ID 508 / 610 mm.

DX52D+Z is a hot-dip galvanized steel coil made to EN 10346 for forming and drawing, not just for flat panels. The grade sits above DX51D in ductility: it tolerates tighter bend radii, deeper draws and more severe roll forming without coating breakdown. QIDAMT supplies DX52D+Z coil slit to your width, with regular or skin-passed surface, chromate-free passivation and oiling on request.

This page covers the chemistry and mechanical limits, the coating masses that are actually stocked, how the coil behaves in slitting, blanking and forming, and the mistakes that turn a good coil into scrap at the press.

What DX52D+Z Coil Is Used For

The Z suffix means hot-dip zinc coating; DX52D is the steel substrate designation. The combination gives a coil that is soft enough to form and strong enough to keep a permanent shape after forming. 일반적인 응용 분야는 다음과 같습니다.:

  • 기기 패널, washing machine shells and refrigerator liners
  • Automotive inner parts, brackets and seat structures
  • Drums, pails, cans and general packaging
  • HVAC components, fan housings and duct fittings
  • Roll-formed profiles, 스터드, frames and shelving
  • Agricultural equipment panels and enclosures

If the part is almost flat and only needs corrosion protection, DX51D+Z is usually sufficient and cheaper. If the part has a deep draw, a sharp bend or a visible formed surface, DX52D+Z reduces the risk of coating cracks and orange peel.

화학적 구성 요소

요소Limit (%)왜 중요한가요?
탄소 (기음)0.12 최대Low carbon keeps ductility high for drawing
규소 (그리고)0.10 최대Controlled for coating adhesion
망간 (망)0.60 최대Strength without hurting formability
인 (피)0.10 최대Higher values embrittle the substrate
황 (에스)0.045 최대Inclusion control
티탄 (의)0.30 최대Stabilises carbon for consistent ageing behaviour

Values are heat-analysis limits under EN 10346; product analysis tolerances apply. For drawing applications, ask for the actual Ti and C values: a heat at the top of the carbon range with little titanium stabilisation will age and can show stretcher strains after forming.

기계적 성질

재산요구 사항실용적인 의미
항복강도 ReH140 – 300 MPaLow yield improves springback control
인장강도 Rm270 – 420 MPaEnough strength for thin panels
신장 A80≥26%Deep drawing and tight bends
Coating massZ100 – Z275 g/m²Z120 for indoor, Z275 for outdoor
코일 내경508 또는 610 mmMust match your uncoiler
코일 무게3 – 10 티Handling and line capacity

The wide yield range is deliberate: DX52D is not a single hardness. Two coils both marked DX52D can differ by 100 MPa in yield, which changes springback and die setup. For critical forming, specify a narrower yield window or ask for a trial coil before committing to a production run.

 -  - 1
Coils leaving the warehouse with protective edge rings — the zinc surface is soft and marks easily during transport.

코팅, Surface and Passivation

Coating mass is quoted as the total on both surfaces. Z275 gives about 275 g/m² 총계, 대충 19 µm of zinc per side. For interior parts Z100 – Z120 is common; for roofing, ducting and outdoor exposure Z275 is the safer choice.

OptionTypical supplyWhen to choose it
코팅Z100, Z120, Z180, Z275Higher mass for outdoor or cut edges
표면레귤러 스팽글 / skin-passedSkin-passed for painting and visible parts
패시베이션Chromate-free / 기름칠한Oiled for storage and forming
가장자리슬릿 엣지 / mill edgeSlit edge for precise width

Skin-passing flattens the surface and removes yield-point elongation, which prevents stretcher strains on formed panels. If the part will be painted after forming, specify skin-passed and oiled material and confirm that the oil is compatible with your pretreatment line.

너비, Thickness and Coil Build

목범위Notes
두께0.3 – 2.0 mm0.4 – 1.2 mm is the common forming range
너비600 – 1250 mmSlit to customer width on request
코일 ID508 / 610 mmState uncoiler mandrel diameter
코일 ODUp to about 1600 mmLimited by container height
코일 무게3 – 10 티Heavier coils suit high-speed lines
Length per coilCalculated from weightConfirm metres before ordering

Always order by thickness, width and metres, not only by tonnes. A heavier coil at the same width gives more metres but also more handling weight; a lighter coil reduces scrap at the end of a run but increases changeover frequency.

슬리팅, Blanking and Forming

Slitting is the first place where a galvanized coil loses value. Burrs on the slit edge expose bare steel and become corrosion initiation points. Use sharp slitter knives with correct clearance, and specify deburred edges for parts that will be handled or painted.

For blanking and pressing, the zinc coating acts as a soft, low-friction layer, which helps drawing but also hides die wear. Keep the die surfaces polished, use a suitable drawing oil and avoid excessive blank holder pressure, which can score the coating.

For roll forming, set the rolls for the actual yield of the coil rather than the nominal grade. Because DX52D covers a wide yield band, a coil at 280 MPa will spring back more than one at 160 MPa, and the same roll setting will not produce the same profile.

Welding and Joining

  • Spot welding is the normal joining method; zinc raises electrode wear, so dress electrodes more often than for cold-rolled steel.
  • For MIG/MAG or TIG, remove zinc from the weld zone first — zinc fumes are harmful and cause porosity.
  • Use zinc-compatible electrodes and adequate fume extraction; never weld galvanized sheet in a confined space without ventilation.
  • Mechanical fasteners and rivets need a coating-friendly washer to avoid damaging the zinc layer.
  • 용접 후, repair the heat-affected zone with a zinc-rich primer.

선택 규칙

DX52D or DX51D?

Choose DX52D when the part is formed: bends under 90°, draws, roll-formed profiles, visible panels. Choose DX51D when the part is flat or lightly bent and cost is the deciding factor. Do not upgrade to DX52D and then design a die that assumes DX51D behaviour — the lower yield of DX52D changes springback.

Which coating mass?

Indoor parts: Z100 – Z120. 집 밖의, roofing and ducting: Z275. Cut edges exposed to weather: higher coating mass or post-cut protection. 해당 부분을 도색할 경우, the coating still matters at scratches; zinc protects the steel at every break in the paint film.

Coil or cut sheet?

Coil suits continuous lines, roll forming and high-volume blanking. Cut sheet suits low volume, prototypes and parts that cannot be run from coil. If you need both, buy coil and have it cut to length rather than ordering two separate stocks.

일반적인 실수

  • Ordering Z275 for an indoor panel and paying for coating that is never needed.
  • Ignoring the yield spread inside the grade, then chasing springback with die adjustments.
  • Using dull slitter knives and accepting a burr that rusts in storage.
  • Welding without removing zinc and without fume extraction.
  • Storing coils on their side or without edge protection, then rejecting the outer wraps.
  • Assuming galvanized coil can be bent to the same radius as cold-rolled steel; the coating limits the tightest radius.

두께, Width and Coil Tolerances

Tolerances follow EN 10143 unless a tighter agreement is written into the order. The values below are the normal supply range; forming lines that run thin gauge at speed often need a tighter thickness window than the standard allows.

목정상적인 공차Tighter option
두께 (0.3 – 2.0 mm)±0.05 mm typical±0.03 mm by agreement
너비 (긴 구멍)±0.5 mm typical±0.2 mm on modern slitters
캠버≤ 5 mm 당 2 중≤ 3 mm for high-speed lines
코일 ID508 / 610 mmFixed, no tolerance needed
코일 무게3 – 10 티Declared per coil
Coating massPer EN 10346 classCertified per coil

Corrosion Behaviour and Storage

아연은 두 가지 방식으로 강철을 보호합니다.: it shields the surface, and it sacrifices itself at scratches and cut edges. That sacrificial action is why a galvanized part keeps working after the paint film is damaged, and why the coating mass, not the paint, sets the service life at edges.

  • Store coils under cover, 바닥에서 떨어져, with ventilation to avoid condensation between wraps.
  • Keep the coil eye clear and never lift on the outer wraps; a crushed wrap becomes scrap.
  • White rust forms when moisture is trapped between wraps — dry the coil and re-wrap before use.
  • Chrome-free passivation plus oil gives the best protection for long sea transit.
  • Do not stack coils on their side for long periods; the edge rings take the load and deform.
 -  - 2
Export coils staged at the port — each eye is protected and the outer wrap carries the handling marks, not the usable inner wraps.

Packing and Delivery

Coils are eye-to-sky or eye-to-wall depending on the container and crane. Each coil is strapped, edge-protected and wrapped for sea transport; desiccant is added for humid destinations. State the lifting method and the maximum coil weight your line can take before shipment.

자주 묻는 질문

Is DX52D+Z the same as DX51D+Z?

아니요. Both are hot-dip galvanized grades to EN 10346, but DX52D has tighter chemistry and better elongation for forming and drawing. DX51D is the general-purpose flat-panel grade.

Can you slit the coil to my width?

예. Send the finished width, tolerance and edge requirement. We slit from master coil and re-wrap with edge protection.

What is the minimum quantity?

One coil for stock sizes; slit widths and special coating masses usually need a small production run. Send your annual volume for the best price.

Does the coil come with a test certificate?

예. Mill test certificate with chemistry, 기계적 성질, coating mass and heat number is standard; 안에 10204 3.1 is available on request.

관련 상품

Need DX52D+Z coil for a forming line?

두께 보내기, 너비, coating mass, coil ID and monthly tonnage. We confirm price, slit tolerance and delivery within 24 시간.

견적을 요청하세요

    개인의사업유통 업체

    답장을 남겨주세요

    메시지를 남겨주세요