S350GD+Z Galvanized Steel Coil
Structural-grade zinc coated coil, 350 الحد الأدنى من العائد MPa, Z275 for frames and outdoor structures.
S350GD+Z is a hot-dip galvanized structural steel coil with a 350 MPa minimum yield strength. It lets a frame, purlin or panel carrier be designed at a thinner gauge than DX51D while keeping the corrosion protection of zinc. QIDAMT supplies S350GD+Z in 0.8–3.0 mm, Z100–Z350, slit to width and packed for export.
The grade is common in steel framing, solar mounting, أجسام الشاحنات, racking and agricultural structures. This page explains the mechanical limits, the coating options, how the higher strength changes forming and welding, and where the grade should not be used.
Where S350GD+Z Coil Is Used
- Light steel framing, ترصيع, joists and wall panels
- Solar mounting rails, brackets and ground-mount structures
- Truck bodies, trailer panels and refrigerated van liners
- Warehouse racking, shelving and mezzanine decking
- Agricultural sheds, livestock equipment and fencing
- HVAC support frames and equipment housings
The economic case is simple: في 350 العائد ميجا باسكال, أ 1.5 mm section can replace a 2.0 mm DX51D section in many bending-dominated parts, saving weight and coating area. The case fails when stiffness, not strength, governs — a thinner gauge flexes more even if the stress is acceptable.
التركيب الكيميائي
| عنصر | حد (%) | دور |
|---|---|---|
| كربون (ج) | 0.20 الأعلى | Strength with weldability |
| السيليكون (و) | 0.60 الأعلى | قوة; too high hurts coating |
| المنغنيز (مينيسوتا) | 1.70 الأعلى | Main strengthening element |
| الفوسفور (ص) | 0.10 الأعلى | Solid solution strengthening |
| الكبريت (س) | 0.045 الأعلى | Inclusion control |
| الألومنيوم (ال) | 0.015 دقيقة | Fine grain and deoxidation |
| ملحوظة + ل | 0.20 الأعلى | Micro-alloying for consistent yield |
The chemistry is designed to reach 350 MPa without the carbon level that would make welding difficult. That is why S350GD can be spot welded and roll formed on equipment used for thinner commercial grades, provided the gauge and current are adjusted.
الخصائص الميكانيكية
| ملكية | متطلبات | ملاحظة التصميم |
|---|---|---|
| Yield strength ReH | ≥350 MPa | Use the certified value, not the minimum |
| قوة الشد جمهورية مقدونيا | 420 - 560 الآلام والكروب الذهنية | Check against connection design |
| استطالة A80 | ≥16% | Enough for normal profiling, not deep drawing |
| كتلة الطلاء | Z100 – Z350 g/m² | Z275 standard for outdoor frames |
| سماكة | 0.8 - 3.0 مم | أقل 0.8 mm forming limits tighten |
| معرف الملف | 508 / 610 مم | Confirm uncoiler capacity |
The tensile range is wide because mills balance strength against elongation. A coil at 540 MPa tensile will form differently from one at 430 الآلام والكروب الذهنية; for roll-formed profiles, ask for a consistent heat and check the first coil before full production.
Coating and Surface Options
| طلاء | الكتلة الإجمالية (جم/م²) | Typical exposure |
|---|---|---|
| Z100 | 100 | داخلي, جاف, رسمت |
| Z180 | 180 | Sheltered outdoor, رسمت |
| Z275 | 275 | الهيكلية في الهواء الطلق, تسقيف, مجاري الهواء |
| Z350 | 350 | Severe exposure, coastal or industrial |
For structural frames that will be painted, Z275 is the usual balance. For coastal sites or uncoated outdoor use, Z350 extends service life. Remember that the coating protects the steel only while it is continuous; حواف مقطوعة, drilled holes and weld zones need a zinc-rich repair coating.
تشكيل, Roll Forming and Welding
S350GD work-hardens more than DX51D, so bending radii should be generous relative to thickness and the bend line should run across the coil width where possible. Springback is higher than commercial grades: a 90° bend may need over-bending of 2 – 4° depending on thickness and tooling.
Roll forming is the natural process for this grade. Set the rolls for the certified yield, keep the strip tension steady and avoid abrupt transitions that can crack the coating at the corners. For profiles with holes, punch before forming only if the distortion is acceptable; otherwise punch after forming.
اللحام: spot welding is standard for thin gauges; for structural joints, use the procedure qualified for the actual thickness and remove zinc from the weld zone. Do not use S350GD as a substitute for a true structural plate in a welded load path without checking the welding procedure and heat input.
قواعد الاختيار
- Match the gauge to the governing case: bending strength, deflection, or local buckling. Higher yield does not improve stiffness.
- Use Z275 as the default for outdoor frames; upgrade to Z350 only where the coating is exposed and unpainted.
- For roll-formed profiles, keep the same heat for a production run so springback does not drift.
- Do not deep draw S350GD; its elongation is adequate for profiling, not for drawing.
- If the part is painted after forming, specify skin-passed, oiled and chromate-free material and confirm paint compatibility.
الأخطاء الشائعة
- Replacing 2.0 mm DX51D with 1.5 mm S350GD and assuming the panel will be as stiff.
- Ignoring springback because the grade is labelled structural.
- Cutting the coil with a dull blade and leaving a burr that rusts first.
- Welding through zinc without fume extraction.
- Mixing S350GD and DX51D parts in the same painted assembly without noting the different surface reactivity.
Corrosion Behaviour and Service Life
The zinc coating protects the steel at scratches, cut edges and fixing points — exactly where painted structural frames fail first. Service life therefore depends on coating mass, exposure category and detailing, not on the yield strength.
- Rural and indoor service: Z100 – Z180 is usually enough when the part is painted.
- Urban, industrial and sheltered outdoor service: Z275 is the practical minimum.
- ساحلية, de-icing salt or ammonia-rich livestock buildings: specify Z350 and inspect cut edges.
- Water traps, unvented box sections and contact with treated timber shorten life regardless of coating mass.
- Dissimilar metals in contact (نحاس, brass, غير القابل للصدأ) cause galvanic attack on the zinc; isolate with a suitable fastener or coating.
Tolerances and Inspection
| غرض | Normal supply | Check before production |
|---|---|---|
| سماكة | ±0.05 mm typical | Measure at three points across the width |
| عرض (شق) | ± 0.5 ملم | Check both ends of the coil |
| احدودب | ≤ 5 مم لكل 2 م | Matters on long roll-formed profiles |
| قوة العائد | ≥350 MPa certified | Compare certificate with trial coil |
| كتلة الطلاء | Z100 – Z350 | Weigh-strip or certificate |
| سطح | Regular / skin-passed | Confirm for painted parts |
Where S350GD+Z Should Not Be Used
- Deep-drawn parts with sharp radii — use DX52D or DX53D instead.
- Heavy welded load paths that require a qualified structural plate procedure.
- Parts where deflection, not stress, governs the design; a thinner high-strength sheet will flex more.
- High-temperature service where zinc coating degrades or embrittles the steel.
Packing and Delivery
Coils are supplied eye-to-sky or eye-to-wall, مربوطة بشرائط فولاذية, edge-protected and wrapped. For container shipment, the coil weight and eye direction must be fixed before booking; a coil that is too large for the door cannot be loaded later. We supply mill certificates, coating mass records and pre-shipment photos.
الأسئلة المتداولة
Is S350GD+Z a structural grade?
نعم. في 10346 defines S350GD with a minimum yield of 350 MPa for structural use. It is not a plate grade and should not be substituted for hot-rolled structural plate in heavy welded connections without engineering review.
What does the Z275 coating mean?
Z275 is a total zinc coating mass of 275 جم/م², عن 19 ميكرومتر لكل جانب. It is the usual choice for outdoor structural parts and roofing.
Can S350GD be galvanized after welding?
The coil is already zinc coated. If the finished part is hot-dip galvanized after fabrication, tell us before ordering so the surface and venting can be planned; double coating is not a substitute for correct detailing.
Do you supply slit widths?
نعم. Send finished width, tolerance and edge condition. Slitting is done from master coil with edge protection on the rewound coil.
منتجات ذات صله
إرسال سمك, عرض, coating mass, profile drawing and tonnage. We confirm price, mechanical certificate and lead time within 24 ساعات.
طلب عرض أسعار
تقدم