3003 لفائف الألمنيوم: حِدّة, Grain and HVAC Fin Stock

3003 aluminium coil is the workhorse alloy of the HVAC and ducting industry. It is an Al-Mn alloy with modest strength, excellent formability and better corrosion resistance than 1100 أو 1060, and it is available in tempers that range from fully soft to stiff enough for fin presses. The coil looks simple: a wound strip of silvery metal. The specification is not. حِدّة, حجم الحبوب, thickness tolerance, coil eye and surface condition all decide whether the material runs through a fin press without tearing or ends up as scrap. This guide explains the alloy, the tempers, the dimensional rules and the selection logic for coil buyers.

ماذا 3003 Aluminium Coil Is and Where It Is Used

3003 is a manganese-bearing aluminium alloy standardised in ASTM B209 and EN 573-3. The manganese addition raises strength by solid-solution and dispersion hardening without the corrosion penalty of copper-bearing alloys. It is not heat-treatable, so strength comes from strain hardening (the H tempers) or from the annealed O condition. The coil is produced by rolling a cast ingot to the required thickness and slitting to width.

The largest use is heat-exchanger fin stock: the thin strip stamped into fins for air conditioners, refrigerators and automotive radiators. The second largest is duct and general sheet for HVAC equipment, kitchen hoods, dryers and ventilation housings. Other uses include roofing and wall cladding, التعبئة والتغليف, لافتات, electrical shielding and marine panels where 5052 is not required.

The alloy is often supplied with a brazing clad layer (3003 + 4045 أو 3003 + 4343) for heat exchangers, or with a conversion coating for corrosion protection. Those variants are separate products; this guide deals with the bare 3003 لفه, because most specification errors start there.

3003 aluminium coils in the warehouse
3003 aluminium coils with eye and wrap: وزن الملف, eye diameter and edge condition determine handling and press loading.

Grade and Chemical Composition

The chemistry of 3003 is narrow enough that most mills hit it without difficulty, but the manganese range is the part that matters. Too little manganese gives a soft coil with low strength; too much can produce coarse constituents and poor surface. Iron and silicon are the main impurities, and they form intermetallic particles that affect grain structure, earing and corrosion behaviour.

عنصر 3003 يتراوح (%) Typical target (%) تأثير
المنغنيز (مينيسوتا) 1.0–1.5 1.20 Solid-solution strengthening; controls grain
السيليكون (و) ≤ 0.60 0.20 النجاسة; affects constituents and brazing
حديد (Fe) ≤ 0.70 0.40 النجاسة; coarse particles reduce formability
نحاس (النحاس) 0.05–0.20 0.10 Small addition improves strength
الزنك (Zn) ≤ 0.10 0.02 النجاسة; keep low for corrosion
التيتانيوم (ل) ≤ 0.10 0.01 Grain refinement if added
Other, each ≤ 0.05 — المجموع ≤ 0.15
الألومنيوم (ال) توازن توازن Matrix

Limits to ASTM B209 / في 573-3. Ask for the actual heat analysis, not a generic data sheet.

The copper range deserves attention. أ 3003 with copper at the low end is slightly softer and easier to braze; at the high end it is stronger but marginally less corrosion-resistant. For fin stock the mill usually targets the middle of the range to balance press performance and sag resistance.

Mechanical Properties by Temper

3003 is supplied in O (صلب), ح14 (quarter hard), ح24 (half hard), H22 and H18 tempers. The temper designation is not decorative: it determines the yield strength, the elongation and the springback in the fin press. A coil ordered in the wrong temper may either tear at the fin die or fail to hold the fin shape after release.

حِدّة قوة الشد (الآلام والكروب الذهنية) قوة العائد (الآلام والكروب الذهنية) استطالة (%) الاستخدام النموذجي
ا (صلب) 110–145 ≥ 40 ≥ 25 رسم عميق, duct work, severe forming
ح14 (quarter hard) 145–185 ≥ 125 ≥ 10 Fin stock, تشكيل عام
ح24 (half hard) 170–210 ≥ 150 ≥ 6 Fin stock, stiff panels
ح22 150–195 ≥ 135 ≥ 8 Intermediate forming
H18 ≥ 200 ≥ 175 ≥ 4 Structural panels, low forming

Typical ranges; exact values depend on thickness and mill practice. Minimums to ASTM B209 apply to the ordered temper.

For fin stock the relevant property is not only strength but sag resistance after brazing. A fin must stay in shape through a brazing cycle at about 600 °ج, where the clad layer melts and the core softens. Grain size and temper both influence sag. A coil with coarse grains sags more; a coil that is too hard cracks in the press. That is why fin stock is usually specified with a grain size range and a temper window rather than a single tensile number.

Dimensions and Tolerances

Coil dimensions are defined by thickness, عرض, القطر الداخلي (eye), outer diameter and weight. Thickness tolerance is the most important for fin stock, because the fin height and the press clearance are set for a nominal gauge. A strip that is 0.02 mm thick at the start and 0.015 mm at the end changes the fin pitch and can jam the die.

المعلمة Common range التسامح النموذجي تعليق
سماكة 0.2–3.0 مم ±0.03 مم (ر < 0.5); ±0.05 مم (t 0.5–1.5) Measure at the coil ends and middle
عرض 100–1500 مم +1.0/0 مم Slit edge quality affects die wear
القطر الداخلي 150, 405, 505 مم ±5 مم Must match the uncoiler mandrel
القطر الخارجي ما يصل الى 1800 مم ±50 مم Limited by coiler and shipping frame
وزن الملف 2–8 ر ±5% Crane and uncoiler capacity
احدودب ≤ 3 مم/م تقاس على طاولة مسطحة Causes strip wander in the press
Edge burr ≤ 0.05 مم Visual and touch Burrs damage the fin die
سطح الانتهاء من مطحنة, no scratches Visual sample Ink marks and oxides cause press marks

Indicative commercial tolerances. Fin stock is often held to tighter thickness and camber limits by the converter.

Coil eye is not a trivial detail. أ 505 mm eye coil is standard for large uncoilers; أ 150 mm eye is common on smaller slitting lines. If the eye is wrong, the coil cannot be mounted, and re-winding adds cost and risk of edge damage. State the uncoiler mandrel diameter in the purchase order, not just the coil weight.

3003 aluminium coil eye and wrapping
Coil eye and wrap condition: the eye must match the uncoiler mandrel, and the wrap must be dry before the coil is stored.

كيف 3003 Coil Is Made

Casting and homogenisation

The alloy is cast into rolling ingots, usually by direct chill casting. The ingot is homogenised at about 580–600 °C to dissolve the manganese and equalise the distribution of constituents. Without homogenisation, the manganese remains segregated, the grain structure is uneven, and the finished coil behaves inconsistently in the press. Homogenisation is a mill process that buyers cannot see, which is why the mill’s process control matters more than the certificate alone.

Hot rolling

The homogenised ingot is hot rolled to a transfer gauge, typically 3–6 مم. Rolling temperature and pass schedule control the recrystallised grain size and the texture. A hot mill that runs too cold produces a harder, less formable strip with a strong directionality.

Cold rolling and annealing

The hot-rolled strip is cold rolled to final gauge, with intermediate annealing as required. The final anneal determines the O temper grain size; the H tempers are produced by controlled cold reduction after the final anneal. For fin stock, the final grain size is usually specified in the range of 20–60 ميكرومتر, because coarse grains reduce sag resistance and fine grains increase press load.

Slitting and packing

The wide coil is slit to customer width. Slitting introduces edge burr and residual stress; a well-set slitter produces a square edge with minimal burr. The coil is then wound on a mandrel, wrapped with paper or film, and packed vertically or horizontally depending on weight. Eye collapse and edge damage in transit are common complaints, so the packing specification should include a wooden or steel eye protector.

قواعد الاختيار

  • Start with the forming operation. Deep drawing and severe bending need O temper; fin pressing needs H14 or H24; flat panels can use H18. Do not order H24 because it is “stronger” if the die was set for H14.
  • Specify grain size for fin stock. Temper alone does not control sag. Ask for the grain size range and the brazing simulation result if the coil will be clad and brazed.
  • Match thickness to the fin die. أ 0.02 mm deviation is small in absolute terms but large relative to a 0.10 mm fin strip. Hold the thickness tolerance tight and check it at both ends of the coil.
  • State the coil eye and weight. The uncoiler mandrel, crane capacity and coil car all depend on these dimensions. A coil that is too heavy for the line is a delivery problem, not a bargain.
  • يختار 5052 أو 3004 when strength or marine corrosion matters. 3003 is not a marine alloy. For salt-water exposure, 5052 أو 5083 is the correct family, و 3003 should not be substituted on price.
  • تأكيد حالة السطح. Fin stock needs a clean, oil-free surface for brazing. Ink marks, oxidation or residual rolling oil cause voids in the brazed joint.

Processing and Handling Rules

3003 coil is easy to handle compared with harder alloys, but it scratches easily and deforms if lifted incorrectly.

  • Lift with a coil hook or a proper coil lifter. A forklift tine under the wrap will crush the edge and create a burr that runs through the entire press run.
  • Keep the coil dry. Water between wraps produces a white oxide stain that is difficult to remove and can interfere with brazing. تخزينها تحت الغطاء, off the floor, with ventilation.
  • Do not remove the wrap until the coil is on the uncoiler. The wrap holds the outer wraps and protects the surface. A coil that has been opened and re-wrapped on site often has edge damage.
  • Check the strip before the first pass. A burr or a bent edge will damage the fin die. Run a short length through by hand and inspect the edge.
  • Control tension on the uncoiler. Too much tension stretches the strip and changes the fin height; too little causes wander and miss-feed.
  • Keep the slit edge away from the die. If the strip has a burr on one side, orient it away from the working face where possible, and replace the slitter blade rather than accept a permanent burr.

Common Misconceptions

“3003 is a marine aluminium”

3003 has good resistance to atmospheric and fresh-water corrosion, but it is not a seawater alloy. Chlorides pit it, especially in crevices and under deposits. Marine service belongs to 5052, 5083 أو 5086, and the price difference is the reason those alloys exist.

“H14 cannot be bent”

H14 bends, but with less elongation and more springback than O temper. It is routinely roll-formed and press-formed. The limitation is the minimum bend radius and the amount of cold work the part can take, not the ability to bend at all.

“Thicker coil is always better”

Thicker strip raises press load, reduces fin density and adds weight and cost. Fin stock is thin for a reason: heat transfer depends on surface area per unit mass. The correct thickness is the one the thermal and mechanical design calls for, not the thickest the mill can roll.

“Aluminium does not oxidise”

Aluminium oxidises immediately in air; the oxide is thin, stable and protective. That is different from rust. The oxide layer can still be damaged by strong alkalis, chlorides and mercury, and a stained coil surface is a sign of moisture or contamination, not of a defective alloy.

Inspection and Receiving Checks

عند الاستلام, check the coil label against the certificate: سبيكة, حِدّة, رقم الحرارة, سماكة, عرض, weight and eye. Measure thickness at the start, middle and end of the coil with a micrometer, and check width at three points. Inspect the outer wrap for damage, the eye for collapse, and the strip edge for burr. Look for water stains, ink marks and oxidation. If the coil is clad for brazing, confirm the clad layer thickness and alloy on the certificate, and keep the coil dry and cool until use.

For fin stock, ask for a grain size report and a sample of the actual coil for a trial press run. A coil that meets the certificate but tears in the die is a process compatibility problem, and it is cheaper to find out on a sample than on a full production run.

التعليمات

ما هو الفرق بين 3003 و 1100?

1100 is commercially pure aluminium with very low alloy content; it is softer, more conductive and weaker. 3003 adds manganese and a little copper, giving higher strength and better formability at a small cost in conductivity. For fins and duct work, 3003 is the stronger choice.

Which temper should I order for fin stock?

H14 or H24 is typical, depending on fin geometry and press capability. The mill and the fin-press supplier should agree the temper and grain size together, because the die was designed around a specific strip behaviour.

يستطيع 3003 be brazed?

نعم. Bare 3003 can be brazed with aluminium filler alloys, and clad 3003 with a 4045 أو 4343 layer is the standard heat-exchanger material. Surface cleanliness and joint design matter more than the alloy choice.

What coil eye diameter should I specify?

Match the uncoiler mandrel: 150 مم, 405 مم و 505 mm are common. Give the mandrel diameter and the coil weight in the enquiry, and state whether the coil will be mounted vertically or horizontally.

How should 3003 coil be stored?

في الداخل, off the ground, جاف, with the wrap intact. Avoid temperature swings that cause condensation, and do not stack coils on their edges without a cradle. Water stains and edge damage are the two most common storage failures.

يكون 3003 suitable for roofing?

نعم, in non-marine atmospheres, provided the coil is supplied in a suitable temper and the roof detail avoids ponding. For coastal roofing, 5052 is the better choice.

يحتاج 3003 aluminium coil for fin stock or duct work?

طلب عرض أسعار

Send alloy, حِدّة, سماكة, عرض, coil eye, weight and grain size requirement to sales@qidamt.com. متعلق ب: 1060 aluminium sheet and plate for plain sheet, أو request a quotation.

QIDAMT supplies aluminium coil and sheet from Shandong, مشتمل 3003, 1060 و 5052 الدرجات. Send the press or forming process with the enquiry; temper and grain size are process decisions, not catalogue numbers.